Tuesday, November 6, 2012

Re: [MW:15866] Re: Piping RF pad Full encirclement sleeve.

Biplab,
 
What;s the line size and branch size, design parameters?
And what's the service?
 
 
Regards,
Ohm-Srinivas

On Tue, Nov 6, 2012 at 10:38 AM, mohd <mohd52100@gmail.com> wrote:
Dear biplab,

My question is that, RF pad welding will cross seam welding of pipe.
Is it acceptable : No Issue.

Ref : sketch API1104 20th edition page :79 B8-B11 for weld sequence details.

regards,
mohd. 



On Sunday, November 4, 2012 2:45:45 PM UTC+3, Biplab Pal wrote:
Dear Exparts,
 
Its very urgent.
We are using carbon steel Welded(Seam) piping Lateral branches. construction code ASME B 31.3
Our client specification says It required full encirclement sleeve pad.
My question is that, RF pad welding will cross seam welding of pipe.
Is it acceptable?
What is the requirement for the acceptance. Please provide code reference for communicare and co-relate.


Thanks & Regards
Biplab Pal
Welding Inspector
E-mail:   bipla...@gmail.com
 
Information in this email and any attachments is confidential and intended solely for the use of the individual(s) to whom it is addressed or otherwise directed. Please note that any views or opinions presented in this email are solely those of the author and do not necessarily represent those of the Company. Finally, the recipient should check this email and any attachments for the presence of viruses. Myself accepts no liability for any damage caused by any virus transmitted by this email.
 

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
 
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
 
 



--
Ohm Guru Namasivaya

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
 
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
 
 

No comments:

[MW:34919] Welder qualification certificate

Dear All     anyone can share a format for welder certificate and card format        Thanks & Best Regards Saleem manhappulath Mob:+9665...