Tuesday, November 6, 2012

Re: [MW:15866] Dissimilar welding CS to DUPLEX SS

Dear Goswami Sir,
 
If its Betweeen SS410/SS430 & Between WCB (A216 Gr.A)
Shall i refer same text Document..
PWHT is advisable or Not..
 
With regards,
Ashish

On Wed, Oct 31, 2012 at 10:58 AM, manpreet <manpreetsin88@rediffmail.com> wrote:
Hi,

I would use E309 for this thickness, no preheating, maximum interpass temperature is 150 deg C


Regards,
Manpreet Singh



On Tue, 30 Oct 2012 14:17:45 +0530 wrote

>Dear Experts,

In our isometric drawing shows dissimilar welding carbon steel to

duplex stainless steel ( 31254 grade ) thk is 9.52 mm. Can anybody

give me guideline to make this WPS.

Regards

Pradip



--

To post to this group, send email to materials-welding@googlegroups.com

To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com

For more options, visit this group's bolg at http://materials-welding.blogspot.com/

http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm



The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.







Catch India as it happens with the Rediff News App. To download it for FREE, click here

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
 
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
 
 

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
 
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
 
 

No comments:

[MW:34920] Tubesheet Hole step

Hello Team, I have one question any tolerance given for tubesheet Hole step. Please do needful. Regards, AP  -- https://materials-...