Dear Mr. Pradip,
As i see your process is GTAW so please go through ASME Sec-IX, 2010, QW-256,see if in your case essential variable or supplimentary essential variables (if impact required) changes as applicable then only you have to change the WPS.
In your case no need to change the WPS.
On Mon, Oct 15, 2012 at 7:26 AM, pradip kumar sil <pradipsil@gmail.com> wrote:
Dear All,
Please Find attached wps . I have one question regarding diameter, it
is not the essential element so diameter wise is it required to
segregate wps.
Secondly, our wps 12, pqr is established in filler wire ER-70S3….. so
can we make the wps ER-70S2 with supporting the pqr –cs-01 because A
No , F No & SFA No is same.
Awaits for your valuable response.
Regards
Pradip
--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
--
Thanks & Regards
Biplab Pal
Welding Inspector
Biplab Pal
Welding Inspector
E-mail: biplab.mech@gmail.com
Information in this email and any attachments is confidential and intended solely for the use of the individual(s) to whom it is addressed or otherwise directed. Please note that any views or opinions presented in this email are solely those of the author and do not necessarily represent those of the Company. Finally, the recipient should check this email and any attachments for the presence of viruses. Myself accepts no liability for any damage caused by any virus transmitted by this email.
Information in this email and any attachments is confidential and intended solely for the use of the individual(s) to whom it is addressed or otherwise directed. Please note that any views or opinions presented in this email are solely those of the author and do not necessarily represent those of the Company. Finally, the recipient should check this email and any attachments for the presence of viruses. Myself accepts no liability for any damage caused by any virus transmitted by this email.
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
No comments:
Post a Comment