Dear Josenit,
 
Please propose 100% RT and 100% DPI...The efficiency of joint still remains the same.
Do let us know the "SERVICE".
 
Regards
Vino, Doha

On Thu, Aug 30, 2012 at 7:42 AM, Josnit <nithindsilva4u@gmail.com> wrote:
Dear Experts,

We have fabricated a vessel of wall thickness 80mm, Construction code is ASME Section VIII Div.2 Ed. 2010. The vessel is cladded with SS 316L. It also has dissimilar weld joints between nozzle (SS) to Shell (CS) Type Category D, this welding was done using ENiCrFe-3 consumables.

My query is :
As per client he requires PA/UT to be done on the category D joints. But as per our NDT subcontractor PA/UT cannot be done for inconel welds, the rays will not penetrate through the welds. Hence requesting you to suggest a suitable method for carrying out the NDT of the same. Is there any technique/Method where we can propose to client, so that NDT can be completed. 

Yours views on the same will higly appreciated,

Regards,
Josenit

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
 
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
 
 

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
 
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
 
 

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...