Dear Tamilselvan,
 

Holes  may be closed with a full-penetration weld using either a welded plug or weld metal. The thickness of the weld and plug shall be greater than or equal to the thickness and  finished weld shall be examined by the magnetic particle or liquid penetrant method in accordance with code. Full volumetric inspection of the weld in accordance with code and shall be performed in addition to any examinations required by the material specification.


 


Thank & Best Regards,

 

M Veera SAMY- Bureau Veritas.

Coimbatore

 

 


 

Date: Mon, 27 Aug 2012 09:12:57 +0400
Subject: [MW:15136] Fwd: WhatType of NDT that shall be performed on plugwelds of cs materials 16mm thick - Reg
From: tamizh74@gmail.com
To: materials-welding@googlegroups.com



Dear all
 
 WhatType of NDT that shall be performed on plugwelds of cs materials 16mm thick

--
With Warm Regards,

S.TAMIZH SELVAN,
Senior Surveyor,
Bureau Veritas India Private Limited,
Bangalore.




--
With Warm Regards,

S.TAMIZH SELVAN,
Senior Surveyor,
Bureau Veritas India Private Limited,
Bangalore.
Mobile: +91-9036056603


--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
 
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
 
 

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...