Re: [MW:15126] WQT Acceptence by UT

Hi
 
I think you have not read ASME Sec IX 2010 edition.
UT can be conducted for Welder qualification now provided the test coupon size is equal to or greater than 13mm as per ASME Sec IX 2010 edition.
 
Regards
 
Prem Nautiyal

--- On Fri, 8/24/12, AJAY KUMAR <ajayengr2k53@gmail.com> wrote:

From: AJAY KUMAR <ajayengr2k53@gmail.com>
Subject: [MW:15120] WQT Acceptence by UT
To: "materials-welding" <materials-welding@googlegroups.com>
Date: Friday, August 24, 2012, 3:42 AM

Dear experts
is there any new ammandmends for welder qualification,where we can
accept UT Test istead of Destructive/RT Test ?

Regards
Ajay Kumar

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm

The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.


--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
 
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
 
 

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...