Re: [MW:15119] Root Gap & Root Face in Pipe Fit Up inspection

You should not reject joint with below mentioned configuration, Specially for pipes welded with GTAW Root. Root Gap of 4 to 5mm and root face of 0.8mm to 0mm is ideal for Piping with GTAW root.

On Wed, Aug 22, 2012 at 10:05 PM, Dindo <dindodelacruz@gmail.com> wrote:
one thing is you could read through the QC Manual of the manufacturer. Different manufacturer have different fit up configuration.


On Wed, Aug 22, 2012 at 6:11 AM, sevak hiren <hirensevak80@gmail.com> wrote:
Dear Experts,

Subject Material: CS/MS Pipes (Dia 2" To 10" x 8 to 10 mm thk) Fit up inspections (As Per ASME B 31.1),

In general WPS root gap is shown as 2 to 3 mm, but practically I have seen that root gap exceeds up to 5 mm in actual fit ups and still proper & full penetration weld is achieved with this much of root gap.

Also welder argues that the root gap is required up to 4 to 5 mm to minimize the contraction of joint after welding.

The same case is with root face that  in WPS root face is shown as around 1.6 mm, but practically I have seen that root face of 0.5 mm only or without root face in actual fit ups and still proper & full penetration weld is achieved.

Although the root gap & root face is a non essential variable as per section IX, but still can we reject the pipe fit ups of root gap of 5 mm & nil root face ?

Can anyone provide some good article / reading material regarding recommendations for pipe fit ups with type of joints & dimensions ?

I need your valuable replies.............

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
 
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
 
 

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
 
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
 
 

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
 
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
 
 

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...