Re: [MW:15113] RE: 15103] electrode with diff impact temp mixing during welding.

Are you doing production impact test? If yes, then that could prove the acceptability of the joint. If no, then you could ask your supplier to give you an MTR for the lot you used that has an impact test results @ -46C (if they have any), electrode manufacturers are the only ones that could do an impact test on all weld metal for the currect ASME code.

On Wed, Aug 22, 2012 at 5:38 AM, pawan <pawan.tiwari@dwekam.org> wrote:
Pl. check impact properties of electrodes at -46deg in same grade of steel
as per SEC-II Part-C.
If it is ok than you can confirm to your client.
Otherwise, go for rework.

-----Original Message-----
From: materials-welding@googlegroups.com
[mailto:materials-welding@googlegroups.com] On Behalf Of mohd
Sent: Wednesday, August 22, 2012 11:46 AM
To: Materials & Welding
Subject: [MW:15103] electrode with diff impact temp mixing during welding.

dear experts,

We have land in difficult situtuation due to welders mistakes.

Electrode E7018H4R impact require -46deg but by mistakes welder used
some electrodes E7018H4R -29deg during welding of 3 long seam 25m
(filling n caping)

Materials      516 gr 60    thk 40t.
Process        GTAW+SMAW

 What could be solution? To save joint.
Client already given cut out.

Regards,
Mohammed.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to
materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at
http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=
anet_ug_hm

The views expressed/exchnaged in this group are members personel views and
meant for educational purposes only, Users must take their own decisions
w.r.t. applicable code/standard/contract documents.



--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm

The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.



--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
 
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
 
 

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...