Re: [MW:15093] Urgent Need for Inconel 625 Material Welder Qualification

for welder qualification as per code you can use Pno. 1 ( carbon steel ) material with Inconel  filler and carry out RT.
regards
vanchi

On Mon, Aug 13, 2012 at 4:17 PM, Shashank Vagal <nach_sam@yahoo.com> wrote:
Test coupon material is not an essential variable for WQT.

--- On Mon, 13/8/12, Kavin Murugam <kavin202082@yahoo.com> wrote:

From: Kavin Murugam <kavin202082@yahoo.com>
Subject: Re: [MW:15074] Urgent Need for Inconel 625 Material Welder Qualification
To: "materials-welding@googlegroups.com" <materials-welding@googlegroups.com>
Date: Monday, 13 August, 2012, 7:59 AM

Any material under P.no 45 will do....
Regards,
Kavin Murugam
0126159644
 

From: "Obidike, Boniface (GE Oil & Gas)" <Boniface.Obidike@ge.com>
To: materials-welding@googlegroups.com
Sent: Wednesday, August 8, 2012 6:17 PM
Subject: [MW:15040] Urgent Need for Inconel 625 Material Welder Qualification

Dear Experts,
 
I want to weld ( cold repair) on H-4 connector made up of Inconel 625 material  and need to qualify my welder for this work. Please, advice best and easy method and materials to use in the welder qualification.
 
Note:  I don't have Inconel 625 material now in my facility and its very scarce in my country, but I have Inconel 625 wire rod for GTAW. Please, also advice other common materials and approach that can go as alternative.   
 
 
"Quality is the Bone, Be the Dog Always"
 
Boniface Obidike
QA/QC Engineer
Speciality Connectors & Pipes
Drilling and Production Systems
GE Oil & Gas Business
Office: +234(1)4629400
Mobile: +2348163479738
Home: +2348039409934
 
 
--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
 
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
 
 


--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
 
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
 
 

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
 
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
 
 

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
 
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
 
 

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...