Mr. Pal,

A WPS is written document and upgraded with actual  parameters used after
successful completion of PQR  tests for the same material and process etc.
i.e., It is mainly focuses the compatibility of a process, filler metal to base metal combination, parameter selection, procedure and other essential, non essential and supplementary (where required)  variables used to make a successful weld.

Once WPS written and is accepted, WPQ is done to check  the skill of the welder operator/tack welder and based up on the that particular successful WPS.

Hence the variables are  less comparatively and an inspector should follow only the variables mentioned under QW 350.

sridhar.
------------------------------------------------------------------------------------------




From: Biplab Pal <biplab.mech@googlemail.com>
To: materials-welding <materials-welding@googlegroups.com>
Sent: Monday, 13 August 2012 6:23 PM
Subject: [MW:15085] requirement of variable for inspection in WQT

Dear Exparts,

I have a doubt on WQT!
Is it required to check all parameters stated in WPS during WQT? Ref:
Sec IX, 2010.

As we know " A WPS is a written qualified welding procedure prepared
to provide direction for making production welds to Code requirements.
The WPS or other documents may be used to provide direction to the
welder or welding operator to assure compliance with the Code
requirements.

Suppose we consider Welder Performance Qualification:
As per QW 350, the essential variables are very few and limited for
each process.

So, what parameters should an Inspector Check during Welder
Performance Qualification as per Sec IX, 2010.
Please give code reference for your statement.

--
Thanks & Regards
Biplab Pal
Mechanical Inspector (PMT)
YASREF Project

E-mail:  biplab.mech@gmail.com

Information in this email and any attachments is confidential and intended
solely for the use of the individual(s) to whom it is addressed or
otherwise directed. Please note that any views or opinions presented in
this email are solely those of the author and do not necessarily represent
those of the Company. Finally, the recipient should check this email and
any attachments for the presence of viruses. Myself accepts no liability
for any damage caused by any virus transmitted by this email.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm

The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.




No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...