Tuesday, August 14, 2012

RE: [MW:15088] Acceptance criteria for Tungsten Inclusion in RT


I found the acceptance criteria for tungsten inclusion which is a rounded indication in Mandatory appendix 4 of ASME Sec. VIII Div.1.
I think Jatin didn't read my question properly as i had clearly mentioned that Construction code was Sec VIII Div.1
 
Regards
 
Prem Nautiyal
 

--- On Mon, 8/13/12, Jean Staton <Jean.Staton@metco-ndt.com> wrote:

From: Jean Staton <Jean.Staton@metco-ndt.com>
Subject: RE: [MW:15084] Acceptance criteria for Tungsten Inclusion in RT
To: "materials-welding@googlegroups.com" <materials-welding@googlegroups.com>
Date: Monday, August 13, 2012, 6:06 PM

Curious, first code reference was ASME VIII, DIV. 1 why did you reference ASME B 31.3?  I am unable to see any reference in ASME VIII that tells me to reference B31.3.  WHY would we go to a piping code when we are on a vessel code in the first place?

 

From: materials-welding@googlegroups.com [mailto:materials-welding@googlegroups.com] On Behalf Of Jatin Dave
Sent: Saturday, August 11, 2012 7:48 AM
To: materials-welding@googlegroups.com
Subject: Re: [MW:15064] Acceptance criteria for Tungsten Inclusion in RT

 

 

Dear Prem,

 

IN ASME B 31.3 Table No. 341.3.2 criteria are  given

 

F    Slag inclusion, tungsten inclusion, or elongated indication
                                             Individual length ≤ T w /3
                                             Individual width ≤ 2.5 mm (3⁄32 in.) and ≤ T w /3
                                             Cumulative length ≤ T w in any 12T w weld length
G           Slag inclusion, tungsten inclusion, or elongated indication
                                              Individual length ≤ 2T w
                                               Individual width ≤ 3 mm (1⁄8 in.) and ≤ T w /2
                                                Cumulative length ≤ 4T w in any 150 mm (6 in.) weld length

Please see Table 

 

Regards

Jatin Dave

9099026886

 


From: joydev dalai <joykolkata07@gmail.com>
To: materials-welding@googlegroups.com
Sent: Friday, 10 August 2012 10:51 AM
Subject: Re: [MW:15053] Acceptance criteria for Tungsten Inclusion in RT

 

Dear Prem,

 

There is nothing cleared about tungsten inclusion, for better information please see in ASME sec.VIII Div.1 ,UW-51 paragraph 

On Thu, Aug 9, 2012 at 9:24 PM, prem nautiyal <prem_nautiyal26@yahoo.com> wrote:

Dear Friends

 

After reviewing a RT film of a Circ.seam joint (16mm thk), which has been welded with TIG + SMAW, i have observed a tungsten inclusion @2-3mm in dia.

The construction code of the vessel is ASME Sec VIII Div.1

 

No doubt this tungsten inclusion is a defect, but i would like to know whether there is any acceptance criteria related to diameter for the same in ASME Sec VIII Div.1. Please give Code reference.

 

Regards

 

Prem Nautiyal

Cell: 9769316004

 

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
 
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
 
 


--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
 
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
 
 

 

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
 
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
 
 


DISCLAIMER: The information contained in this e-mail may be confidential and is intended solely for the use of the named addressee. Access, copying or re-use of the e-mail or any information contained therein by any other person is not authorized. If you are not the intended recipient please notify us immediately by returning the e-mail to the originator.
--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
 
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
 
 

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
 
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
 
 

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...