[MW:15160] RE: 15156] Is Sulphur segregation reason for reject a PQR?

Tugrulhan,
 
Sulphur segregation test is only a supplemental test. It's either a client or any project or any service application specific requirement. Failure of such test would not fail an ASME Sec-IX PQR. You need to clarify what's being asked in the design or project specification and decide accordingly.Usually such tests are asked for the base metals not for welds.
 
Thanks. 
 

Pradip Goswami,P.Eng.IWE

Welding & Metallurgical Specialist

Ontario, Canada.

Email-pgoswami@sympatico.ca,

pgoswami@quickclic.net

 


From: materials-welding@googlegroups.com [mailto:materials-welding@googlegroups.com] On Behalf Of tugrulhan özdemir
Sent: Wednesday, August 29, 2012 11:05 AM
To: materials-welding@googlegroups.com
Subject: [MW:15156] Is Sulphur segregation reason for reject a PQR?

Hello dear people



I  saw a sulphur segregation on a macro test photos. Is this a reason for reject a PQR? Tensile test  bend test   notch toughness test  RT   and Hardness tests are OK.


Thank yok



Tugrulhan OZDEMIR
 

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
 
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
 
 

No comments:

[MW:35692]

Dear all    Can I do MPI above painting surface for cs  tank  Regards, Sriram Srinivasan -- https://materials-welding.blog...