Sunday, August 26, 2012

[MW:15134] Re: P-T Curves

These Pt - T curves are different of ASMEB B16.5 curves? Or equivalent?


On Sunday, August 26, 2012 10:55:20 AM UTC-5, himan wrote:
Dear Experts

Would you please share some information/references regarding P-T curves in pressure vessels?

Regards,
Himan Nikdin

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
 
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
 
 

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...