Saturday, July 14, 2012

Re: [MW:14863] Duplex SS to 516 Grade 70 welding - COnsumbale

I suggest ERNiCr3 for root and hot; and ERNiFe-3 for fill and cap.
Sent from my BlackBerry® wireless device

From: "fredric" <fredric.prabu@bwgindia.com>
Sender: materials-welding@googlegroups.com
Date: Wed, 11 Jul 2012 14:56:06 +0530
To: <materials-welding@googlegroups.com>
ReplyTo: materials-welding@googlegroups.com
Subject: [MW:14843] Duplex SS to 516 Grade 70 welding - COnsumbale

Dear Experts

 

Kindly suggest suitable welding consumable (GMAW & GTAW) for dissimilar welding.

 

Pls suggest suitable consumable to weld duplex stainless steel (DIN 1.4462 or ASTM 31803) to carbon steel (ASTM A516 gr 70)

 

Regards

Fredric Prabu. k

No comments:

Re: [MW:35289] Welding consumable for S355J2WP material

S355 J2 WP  is a weathering structural steel  It has better atmospheric corrosion resistance. Use E 8018 - W1/W2  Electrodes This is regular...