Thursday, July 12, 2012

Re: [MW:14854] Heating/cooling rate requirement for PWHT

Aakar,
Is there any ASME interpretation to clarify on this non-mandatory requirement.You know,our custom ask us to provide documentary proof to prove our explanation right. 

Regards,
Devin

在 2012年7月12日星期四UTC+8下午2时27分43秒,aakar写道:
Yes it is not mandatory,it is very clearly stated that need not to less than 56 c/hr without any structural damages

-original message-
Subject: [MW:14846] Heating/cooling rate requirement for PWHT
From: Devin <yanfeixiu@gmail.com>
Date: 12-07-2012 8:39 am



Dear All,

As per ASME section Ⅲ NX-4623,Above 800°F(425℃) the rate of heating and
cooling in any hourly interval shall not exceed 400°F(222℃)divided by the
maximum thickness in inches of the material being heat treated,but shall
not exceed 400°F(222℃)and *need not to be less than 100**°F(56**℃)in an
hourly interval.*

 

Now the actual heating and cooling rate in our production we made is 50℃/hour
which is less than 56℃/hour required above. Our custom insist that this is
unacceptable and should be reheated. But my understanding is that the *56**℃is not a mandatory requirement
*and only the upper limitation is required. Do I understand this correctly?
PLZ guide me! Appreciate it!

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

[MW:34920] Tubesheet Hole step

Hello Team, I have one question any tolerance given for tubesheet Hole step. Please do needful. Regards, AP  -- https://materials-...