Re: [MW:14820] Impact test qualification requirement for WPS/PQR

dear alll,
      can we able to combine two pqr's ,one with impact test and the other without impact test?

On Fri, Jul 6, 2012 at 10:49 PM, John Henning <jhenning@deltak.com> wrote:

Ah, but there is a catch.  All essential and supplementary essential variables must be the same.  While technically feasible, it is difficult to pull off.  If nothing else, heat inputs will usually be vastly different between the thick and the thin coupons.  About the only place I see this working is with machine (automatic) GTAW or another machine process.  For a manual processes like SMAW it is unlikely that heat input will be the same.

 

John A. Henning

Welding & Materials

 

From: materials-welding@googlegroups.com [mailto:materials-welding@googlegroups.com] On Behalf Of gogulu kumar
Sent: Friday, July 06, 2012 1:58 AM
To: materials-welding@googlegroups.com
Subject: Re: [MW:14780] Impact test qualification requirement for WPS/PQR

 

Dear John A. Henning,

 

With reference to below interpretation, PQR 2 should be acceptable for depositing 21mm thick weld by SMAW process and 

PQR 1 & PQR 2 can support a WPS with notch toughness requirement (at -18 deg. C) with base metal thickness range from 10mm to 80mm and weld metal deposited by SMAW process up to 38mm max.

 

Please correct me if i am wrong.

 

Thanks & Regards

Gogulu Kumar

 

 

On Thu, Jul 5, 2012 at 8:30 PM, John Henning <jhenning@deltak.com> wrote:

This is incorrect,  for PQR 2, QW-451.1 limits the maximum thickness of base metal and weld metal to 2T and 2t, respectively.  Therefore, PQR 2 is only qualified to a maximum of 20mm base metal thickness and 16mm SMAW weld metal thickness.  Since PQR 1 was impact tested at a higher temperature than required it is not applicable to welding on this combination of materials and required MDMT.

 

John A. Henning

Welding & Materials

 

From: materials-welding@googlegroups.com [mailto:materials-welding@googlegroups.com] On Behalf Of gogulu kumar
Sent: Wednesday, July 04, 2012 12:11 PM
To: materials-welding@googlegroups.com
Subject: Re: [MW:14764] Impact test qualification requirement for WPS/PQR

 

Dear Asad Azmi,

 

PQR 2 can be used to deposit 21mm thick weld if other essential and supplementary essential variables are same as PQR 1, since "T limits impact" (QW-403.6) has limitation only on min. thickness qualified.

 

Regards

Gogulu Kumar 

 

On Wed, Mar 14, 2012 at 4:01 PM, asad azmi <azmiasadayub@gmail.com> wrote:

Dear All,

 

Greetings.

 

A vessel is being fabricated as per ASME SEC VIII DIV 1.

 

Vessel material is SA 387 GR 12 CL2, 65 THK. MDMT is   -18 DEG CELCIUS.

 

Approved WPS is supported by  2 PQR  detailed as below --

 

PQR 1

 

Test coupon thickness - 40 mm ,

Welding process used - GTAW + SMAW + SAW ,

Weld deposit by SMAW  Process is 19 mm.

Weld deposited by SMAW  is impact tested at   0 deg celcius.

 

PQR 2

 

Test coupon thickness - 10 mm ,

Welding process used - GTAW + SMAW ,

Weld deposit by SMAW  Process is 8 mm.

Weld deposited by SMAW  is impact tested at    - 18 deg celcius.

 

Whether  PQR  2 can be used for SMAW  Process to deposit  21 mm weld in a weld groove of 65 mm in depth .( for closing seam of shell to dished head & nozzle to dished  head weld seam)

 

Please advice. please give ASME SEC IX Reference.

 

Thanks & Regards

 

Asad Azmi

 

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.



 

--

Regards

Gogulu Kumar

 

 

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.


______________________________________________________________________
The information in this email is confidential, and is intended solely for the addressee(s). If you are not the intended recipient of this email please let us know by reply and then delete it from your system; you should not copy this message or disclose its contents to anyone. The internet can not guarantee the integrity of this message. HAMON (and its subsidiaries) shall (will) not therefore be liable for the message if modified.
______________________________________________________________________

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.



 

--

Regards

Gogulu Kumar

 

 

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.


______________________________________________________________________
The information in this email is confidential, and is intended solely for the addressee(s). If you are not the intended recipient of this email please let us know by reply and then delete it from your system; you should not copy this message or disclose its contents to anyone. The internet can not guarantee the integrity of this message. HAMON (and its subsidiaries) shall (will) not therefore be liable for the message if modified.
______________________________________________________________________

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

[MW:34920] Tubesheet Hole step

Hello Team, I have one question any tolerance given for tubesheet Hole step. Please do needful. Regards, AP  -- https://materials-...