Dear fre,

suitable filler Wire ER 90S - B3, pls refer in ASME sec IIC.

On Sun, Jul 8, 2012 at 1:56 PM, Bijay <bkchoudhury80@yahoo.com> wrote:
Dear Experts,

Kindly suggest me which filler wire best suitable for dissimilar metal pipe joints P22 to cs SA106 Gr B

Awaiting for your valuable answer
 
With Regards

Bijay Kumar Choudhury
Mob +91 94084 43554
Mob +91 89806 30973

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

[MW:34920] Tubesheet Hole step

Hello Team, I have one question any tolerance given for tubesheet Hole step. Please do needful. Regards, AP  -- https://materials-...