Re: [MW:14774] Thickness of transverse Root Bend & Face Bend test Specimen

Dear hiren,
As per ASME Sec-IX,
The thickness of the face bend and root bend shall be the same as of test coupon.
Only thing is the machining allowances in order to make the specimens flat shall be deducted.

Regards
Shadab ansari

On Jul 5, 2012 7:13 PM, "sevak hiren" <hirensevak80@gmail.com> wrote:
Dear Experts,
 
For a WPS qualification test made on 15 mm thk. SA 516 Gr.60 plate,
 
What would be the required final thickness for transverse Root Bend & Face Bend test Specimen as per ASME Section IX ?
 
As per figure QW-462.3(a) it must be 10 mm, am I correct ?

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

[MW:34919] Welder qualification certificate

Dear All     anyone can share a format for welder certificate and card format        Thanks & Best Regards Saleem manhappulath Mob:+9665...