DEAR EXPERTS
 
WPS FOR GTAW + SMAW PROCESS & SUPPORTING PQR (1) FOR GTAW 6" DIA PIPE HAVING 7.11MM THICK AND (2) PLATE HAVING 20 MM THICKNESS IS 2062 GR.B MATERIAL.
 
PIPE THICKNESS 1.5 -20 MM RESTRICTED
 
WPS QUALIFIED FOR GTAW-3MM AND SMAW 24.11MM THICKNESS,  CAN WE ACCEPTED THIS ONE OR NOT. 

--