Tuesday, June 19, 2012

Re: [MW:14590] MOC for sodium ortho silicate

Ammar,
I have known this chemical used in some glass manufacturing industries is mostly stored in MS drums. MS is ok for this highly alkaline chemical.
S Vagal

--- On Mon, 18/6/12, nandakumar pandit <panditns1@gmail.com> wrote:

From: nandakumar pandit <panditns1@gmail.com>
Subject: Re: [MW:14583] MOC for sodium ortho silicate
To: materials-welding@googlegroups.com
Date: Monday, 18 June, 2012, 6:57 AM

U can use MS without problem of corrosion.

regards
nspandit

On Sun, Jun 17, 2012 at 1:34 PM, Ammar Shaikh <ammar.ali.shaikh@gmail.com> wrote:
Dear Experts,

Good Day.

Can anyone suggest the material of construction for Alkali, Sodium Ortho silicate (Na4SiO4).

I want to know whether mild carbon steel is ok or not


Ammar Shaikh

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.



--
N. S. Pandit
alternative e-mail panditns1@rediffmail.com


--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

Re: [MW:35289] Welding consumable for S355J2WP material

S355 J2 WP  is a weathering structural steel  It has better atmospheric corrosion resistance. Use E 8018 - W1/W2  Electrodes This is regular...