Monday, June 4, 2012

Re: [MW:14463] Branch connection procedure required

Dear Ahmed,
 
Please refer to Para 304.3 of ASME B31.3 - 2002 Ed.
 
Ammar

On Sun, Jun 3, 2012 at 10:57 PM, ahmed <eng_ahmed450@yahoo.com> wrote:
Dear All Good Day
I want Branch connection procedure or calculations sheet for the
following variables

Variables           Run Pipe                          Branch Pipe

Material         API 5L Gr B (Spiral)          API 5L Gr B
(Spiral)

Diameter            48" (1200mm)               28" (700mm)

Thickness                9.5                                 9.5

Pressure                                 16 bar

Temperature                            70 C

Fluid                                       Water




          Ahmed Gomaa
          Sr QA/QC Eng
Cswip3.1,CWI,API570,ISO 9001:2008
         Ajyad Project
   MAKKAH-HOLY HARAM
       00966 593298850




--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

Re: [MW:35289] Welding consumable for S355J2WP material

S355 J2 WP  is a weathering structural steel  It has better atmospheric corrosion resistance. Use E 8018 - W1/W2  Electrodes This is regular...