Sunday, June 3, 2012

[MW:14452] flange material inspection

Dear Freinds ,
 
I want to know how we can distinguish that a flange has made by plate or has made by forged material . what's the meathods . 
 
is it possible by comparing sound velosity by ultrasonic test .
 
Best regards
A. Alavi 

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

[MW:35754] interpration

  Interpretation #: BPV IX-18-34  Record Number: 18-771  Subject Description: SC IX; QW-401.1 and QW-403.6 - Thickness Range Qualified for I...