Dear friend,
 
As per an asme 9 there is provosion if any welder is qualified with V groove,he is qualifiy an fillet weld as it no full penetration .But need to check an project specifications scope requirnments.
 
i hope your query is clarified.
 
regards
 
dinesh

On Mon, May 28, 2012 at 8:20 AM, Sam Malemela <smalemela@spc.co.za> wrote:

Hi Colleagues,

 

I am working on a pipeline construction project in Mpumalanga –South Africa. The client is a reputable water utility company in South Africa who has appointed a contractor to construct 37 km of 610mm Diameter pipeline. The joint design is Partial Joint Penetration ( by means of fillet weld). The pipe fit up is spigot and socket joint.

 

The appointed inspection authority is refusing to accept welder qualification for 'v' grove joint design allegedly because the client specification has asked for fillet weld and NOT butt weld.

 

Requalification of welders is not an issue apart from the time it will take to set up and get the qualification test done. I also know from training that range of approval for grove includes fillet welds as well.

 

Should I simply re-qualify the welders although their qualification covers fillet welds if range of approval is considered or should I insist on the inspection authority consulting for proper information on this matter?

 

The integrity of the profession is under threat if people without proper knowledge are allowed to rewrite the specifications for the industry and go unchallenged.

 

Your urgent response will be greatly appreciated.   

 

MALEMELA  N. S.

SITE MANAGER

SOUTHERN PIPELINE CONTRACTORS

6 Main Reef Road

DUNSWART

1508

TEL:0119148519

FAX:0119144524

CELL:0823892592

www.spc.co.za

 

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

Comments

Popular posts from this blog

Heat tint (temper) colours on stainless steel surfaces heated in air // Heat tint

Introduction The colour formed when stainless steel is heated, either in a furnace application or in the heat affected zone of welds, is dependent on several factors that are related to the oxidation resistance of the steel. The heat tint or temper colour formed is caused by the progressive thickening of the surface oxide layer and so, as temperature is increased, the colours change.   Oxidation resistance of stainless steels However, there are several factors that affect the degree of colour change and so there is no a single table of colour and temperature that represents all cases. The colours formed can only be used as an indication of the temperature to which the steel has been heated. Factors affecting the heat tint colours formed Steel composition The chromium content is the most important single factor affecting oxidation resistance. The higher the chromium, the more heat resistant the steel and so the development of the heat tint colou...

[MW:5202] RE: 5200] NDT after PWHT

------------------------------------- Interpretation:  I‑89‑14 Subject:         Section I (1986 Edition, 1987 Addenda), PW‑11,                  NDE Prior to PWHT Date Issued:     December 15, 1988 File:            BC88‑393   Question: Does PW‑11 require that NDE be performed on welds after they have been subjected to the postweld heat treatment required by PW‑39?   Reply: No, unless the conditions described in PW‑11.2.2 exist. ---------------------------------------------- Interpretation:  VIII-1-98-09 Subject:         Section VIII, Division 1 (1995 Edition, 1996 Addenda); NDE                 ...

Materails FAQs

Q: What are equivalents for standard Q 235 B (and Q 235 A) for U-channels? (asked by: boris.vielhaber@vait.com) A: DIN Nr. = 2393 T.2, 2394 T.2, EN 10025 W. Nr. DIN 17007 = 1.0038 Design DIN 17006 = RSt 37-2, S235JRG2 (Fe 360 B) Q: What is St DIN 2391 BK material? (asked by: dmcandrews@automaticstamp.com) A: Precision steel tubes, cold-finished/hard. Q: What is C.D.W. Boiler Tube? (asked by: montydude123@yahoo.com) A: Cold Drawn Welded Boiler Tube. Q: WHAT IS W.Nr. 1.4301? PLS TELL US IN EASY LANGUAGUE (asked...