Skip to main content

RE: [MW:14418] Code & Standard for Tubing

Remember you can't judge depth with a radiograph.

-----Original Message-----
From: materials-welding@googlegroups.com [mailto:materials-welding@googlegroups.com] On Behalf Of Vu Duc Thuan
Sent: Wednesday, May 30, 2012 1:38 AM
To: materials-welding@googlegroups.com
Subject: RE: [MW:14413] Code & Standard for Tubing

Dear All,

Thanks for your supporting,
that mean, we will check RT films and the densities of RT film to be measured at both weld metal and base metal location, it should compared the densities result as per B31.3 table 341.3.2


Regards,

Vu Duc Thuan
Email: dthuan117@gmail.com
Mobile: +84 983 017 936
Sky: vdthuan_vtau

-----Original Message-----
From: materials-welding@googlegroups.com
[mailto:materials-welding@googlegroups.com] On Behalf Of sankar bombay
Sent: Wednesday, May 30, 2012 11:40 AM
To: materials-welding@googlegroups.com
Subject: Re: [MW:14408] Code & Standard for Tubing

Dear friend,
B31.3 there have given teh acceptance for the root concavity check
table:341.3.2
check the density of the root and parrent material.. its should not
more than parent materialn at concavity side ( lenght is not given we dont
want to considered )
API 510 we have accpetance its should not be more 6mm lengh of
concavity
depth same

Regards
sankar.k

On 5/30/12, Vu Duc Thuan <dthuan117@gmail.com> wrote:
> Dear Expert,
>
>
>
> In my project, we have some tubing line ( ½" SS316L and Duplex) need
> to weld with reducer same material, we have WPS for both of material.
> The problem is the RT report show internal concavity but we do not
> have accept criteria for those weld joints as per drawing, Spec..etc..
>
>
>
> Kindly please advise which code & standard are using for the tubing. (
> tubing fix on the hydraulic control panel )
>
>
>
>
>
> Regards,
>
>
>
> Thuan
>
> --
> To post to this group, send email to
> materials-welding@googlegroups.com
> To unsubscribe from this group, send email to
> materials-welding+unsubscribe@googlegroups.com
> For more options, visit this group's bolg at
> http://materials-welding.blogspot.com/
> The views expressed/exchnaged in this group are members personel views
> and meant for educational purposes only, Users must take their own
> decisions w.r.t. applicable code/standard/contract documents.
>


--
shankar

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to
materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at
http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and
meant for educational purposes only, Users must take their own decisions
w.r.t. applicable code/standard/contract documents.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

DISCLAIMER: The information contained in this e-mail may be confidential and is intended solely for the use of the named addressee. Access, copying or re-use of the e-mail or any information contained therein by any other person is not authorized. If you are not the intended recipient please notify us immediately by returning the e-mail to the originator.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

Comments

Popular posts from this blog

Materails FAQs

Q: What are equivalents for standard Q 235 B (and Q 235 A) for U-channels? (asked by: boris.vielhaber@vait.com) A: DIN Nr. = 2393 T.2, 2394 T.2, EN 10025 W. Nr. DIN 17007 = 1.0038 Design DIN 17006 = RSt 37-2, S235JRG2 (Fe 360 B) Q: What is St DIN 2391 BK material? (asked by: dmcandrews@automaticstamp.com) A: Precision steel tubes, cold-finished/hard. Q: What is C.D.W. Boiler Tube? (asked by: montydude123@yahoo.com) A: Cold Drawn Welded Boiler Tube. Q: WHAT IS W.Nr. 1.4301? PLS TELL US IN EASY LANGUAGUE (asked...

[MW:36169] Cold Bending Qualification

Dear Experts,  Can anyone share the inspection requirements or a qualification procedure for cold bending? Our client spec states only the requirements for induction bending and would like to know your opinion on the cold bend inspection requirements. The code of construction is B31.3, Max. 5D bends, A106 SS 316L.  Thanks in Advance. -- https://materials-welding.blogspot.com/ https://www.linkedin.com/groups/122787 --- You received this message because you are subscribed to the Google Groups "Materials & Welding" group. To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com . To view this discussion visit https://groups.google.com/d/msgid/materials-welding/1be61cc3-e9c9-4a5f-834d-e8485e248432n%40googlegroups.com .

Heat tint (temper) colours on stainless steel surfaces heated in air // Heat tint

Introduction The colour formed when stainless steel is heated, either in a furnace application or in the heat affected zone of welds, is dependent on several factors that are related to the oxidation resistance of the steel. The heat tint or temper colour formed is caused by the progressive thickening of the surface oxide layer and so, as temperature is increased, the colours change.   Oxidation resistance of stainless steels However, there are several factors that affect the degree of colour change and so there is no a single table of colour and temperature that represents all cases. The colours formed can only be used as an indication of the temperature to which the steel has been heated. Factors affecting the heat tint colours formed Steel composition The chromium content is the most important single factor affecting oxidation resistance. The higher the chromium, the more heat resistant the steel and so the development of the heat tint colou...