Hi

Dear i am not asking about some one's trade secret or any formulation.
i am just asking that is there any possibility to use MMA flux in FCAW wires.
if there is any feasibility the what is the procedure. share with me some ideas how to research on this topic as i am assigned by my CEO.
hopefully you got my point.
Thanks


From: prem nautiyal <prem_nautiyal26@yahoo.com>
To: "materials-welding@googlegroups.com" <materials-welding@googlegroups.com>
Sent: Thursday, May 24, 2012 8:37 PM
Subject: Re: [MW:14353] Inquiry about the flux of a flux cored wire

Hi
 
No you cannot just blindly use the flux of MMA electrodes in FCAW.
 
However Some minerals are common for FCAW and SMAW.
 
You are talking about the formulation part of FCAW wires and SMAW electrodes which is the trade secret of any consumable manufacturer and no one will share it with you on this open forum.
 
This is not the forum for discussing this topic and you will not come across any consumable formulation on the internet !
If you are interested in knowing the general formulation of consumables please refer the following book: Fluxes, Solders and Welding Alloys by Louis F Martin.
 
Just for your information SMAW electrodes coating contain fluorides, carbonates, slag forming ingredients, deoxidisers, iron powder and alloying ingredients bonded with potassium/sodium/lithium silicates.
For example a rutile electrode coating will consist of Manganese dioxide, rutile, alumina, fluoride, ferrosilicon, ferromanganese, iron powder, etc.
 
Similarly a self shielded FCAW wire fill may contain SiO2, iron powder, CaCO3, Mn, CaF2, etc..
 
 
Regards
 
Prem Nautiyal

From: "murtaza506@yahoo.com" <murtaza506@yahoo.com>
To: Materials & Welding <materials-welding@googlegroups.com>
Sent: Thursday, May 24, 2012 4:44 PM
Subject: [MW:14352] Inquiry about the flux of a flux cored wire

can we use the flux of MMA welding electrodes in flux cored wire??
if yes then please tell me how we can do so??
please share some links or data carrying such information.
thanks

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.


--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.


Comments

Popular posts from this blog

Materails FAQs

Q: What are equivalents for standard Q 235 B (and Q 235 A) for U-channels? (asked by: boris.vielhaber@vait.com) A: DIN Nr. = 2393 T.2, 2394 T.2, EN 10025 W. Nr. DIN 17007 = 1.0038 Design DIN 17006 = RSt 37-2, S235JRG2 (Fe 360 B) Q: What is St DIN 2391 BK material? (asked by: dmcandrews@automaticstamp.com) A: Precision steel tubes, cold-finished/hard. Q: What is C.D.W. Boiler Tube? (asked by: montydude123@yahoo.com) A: Cold Drawn Welded Boiler Tube. Q: WHAT IS W.Nr. 1.4301? PLS TELL US IN EASY LANGUAGUE (asked...

[MW:36169] Cold Bending Qualification

Dear Experts,  Can anyone share the inspection requirements or a qualification procedure for cold bending? Our client spec states only the requirements for induction bending and would like to know your opinion on the cold bend inspection requirements. The code of construction is B31.3, Max. 5D bends, A106 SS 316L.  Thanks in Advance. -- https://materials-welding.blogspot.com/ https://www.linkedin.com/groups/122787 --- You received this message because you are subscribed to the Google Groups "Materials & Welding" group. To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com . To view this discussion visit https://groups.google.com/d/msgid/materials-welding/1be61cc3-e9c9-4a5f-834d-e8485e248432n%40googlegroups.com .

Heat tint (temper) colours on stainless steel surfaces heated in air // Heat tint

Introduction The colour formed when stainless steel is heated, either in a furnace application or in the heat affected zone of welds, is dependent on several factors that are related to the oxidation resistance of the steel. The heat tint or temper colour formed is caused by the progressive thickening of the surface oxide layer and so, as temperature is increased, the colours change.   Oxidation resistance of stainless steels However, there are several factors that affect the degree of colour change and so there is no a single table of colour and temperature that represents all cases. The colours formed can only be used as an indication of the temperature to which the steel has been heated. Factors affecting the heat tint colours formed Steel composition The chromium content is the most important single factor affecting oxidation resistance. The higher the chromium, the more heat resistant the steel and so the development of the heat tint colou...