Re: [MW:14372] Acceptance criteria for welding of Cupro-Nickel pipe

Hi!
Instead of Using 70:30CuNi use 90:10 CuNi wire with Pulse Tig ,Up slope /down slope welding facilty and ensure proper purging of thye weld , Use higher dia Ceramic Cup
 
Regards
 
Hegde

--- On Mon, 28/5/12, Anil Hegde <nottyanil@gmail.com> wrote:

From: Anil Hegde <nottyanil@gmail.com>
Subject: Re: [MW:14369] Acceptance criteria for welding of Cupro-Nickel pipe
To: materials-welding@googlegroups.com
Date: Monday, 28 May, 2012, 10:11 AM

Mr Megnath ,
 
Kindly clean the joint surface by buffing wheel  & then take RT .
 
It will get cleared
 
Regards
Anil Hegde
 
 
On Sat, May 26, 2012 at 11:57 AM, Megnath <megnath@gmail.com> wrote:
Dear friends,
We are doing welding (GTAW using 99.99% Argon & 70-30 cnsumable) of
CuNi - 90-10 pipe and all of them fall under class 1 pipe and forced
to examine the weld by Radiograpy. On review of radiograph, none of
the joint gets cleared. The only problem with welding is "POROSITY".
As pe our contract, the size of permissible porosity is 0.2t
(thickness of pipe is 3,4mm) and even 1mm porosity calls for repair.
Could any one share your knowledge on the following.
1. Acceptance criteria for RT of CuNi pipe weld
2. How to overcome from the porosity

Best Regards,
Megnath

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

Comments

Popular posts from this blog

Heat tint (temper) colours on stainless steel surfaces heated in air // Heat tint

Introduction The colour formed when stainless steel is heated, either in a furnace application or in the heat affected zone of welds, is dependent on several factors that are related to the oxidation resistance of the steel. The heat tint or temper colour formed is caused by the progressive thickening of the surface oxide layer and so, as temperature is increased, the colours change.   Oxidation resistance of stainless steels However, there are several factors that affect the degree of colour change and so there is no a single table of colour and temperature that represents all cases. The colours formed can only be used as an indication of the temperature to which the steel has been heated. Factors affecting the heat tint colours formed Steel composition The chromium content is the most important single factor affecting oxidation resistance. The higher the chromium, the more heat resistant the steel and so the development of the heat tint colou...

[MW:5202] RE: 5200] NDT after PWHT

------------------------------------- Interpretation:  I‑89‑14 Subject:         Section I (1986 Edition, 1987 Addenda), PW‑11,                  NDE Prior to PWHT Date Issued:     December 15, 1988 File:            BC88‑393   Question: Does PW‑11 require that NDE be performed on welds after they have been subjected to the postweld heat treatment required by PW‑39?   Reply: No, unless the conditions described in PW‑11.2.2 exist. ---------------------------------------------- Interpretation:  VIII-1-98-09 Subject:         Section VIII, Division 1 (1995 Edition, 1996 Addenda); NDE                 ...

Materails FAQs

Q: What are equivalents for standard Q 235 B (and Q 235 A) for U-channels? (asked by: boris.vielhaber@vait.com) A: DIN Nr. = 2393 T.2, 2394 T.2, EN 10025 W. Nr. DIN 17007 = 1.0038 Design DIN 17006 = RSt 37-2, S235JRG2 (Fe 360 B) Q: What is St DIN 2391 BK material? (asked by: dmcandrews@automaticstamp.com) A: Precision steel tubes, cold-finished/hard. Q: What is C.D.W. Boiler Tube? (asked by: montydude123@yahoo.com) A: Cold Drawn Welded Boiler Tube. Q: WHAT IS W.Nr. 1.4301? PLS TELL US IN EASY LANGUAGUE (asked...