Skip to main content

Re: [MW:13317] RE: 13288] To increase hardness of Heat Exchanger fin

Dear Priyanka,
                    You may try coating the fins material with Plasma Nitriding or CN or DLC Coating. Will provide the details once you confirm the material.

2011/12/26 Priya Deshmukh <piyuwillseeu@gmail.com>
Dear Sir,

More hardness of the fin is required because it is used in heat
recovery of exhaust gases having abrasive particles in it.

The temperature might be around 450 deg. C and particles are abrasive
eroding the fin surface.

Please reply if you have some solution.

Thanks & Regards,

Priyanka Deshmukh

On 12/26/11, pgoswami <pgoswami@quickclic.net> wrote:
> Hi Priyanka,
>
> What are the design conditions for the air cooled finned exchangers, e.g
> operating media, design temperature , materials of construction? .Is the
> intended application is for refinery or other type of plants ?
>
> Generally  pure aluminum is popular as fin material, however it does not
> offer much scope for improvement of hardness as this this material  is not
> heat treatable. Improvement of hardness through surface coating or thermal
> spray may impair corrosion resistance and the heat transfer coefficient.
>
> Below are some extracts on recommended material of construction for fin
> tubes, typically for oil and gas applications from various appropriate
> specifications.
>
> Thanks
>
>
> Pradip Goswami,P.Eng.IWE
> Welding & Metallurgical Specialist & Consultant
> Ontario,Canada.
> Email-pgoswami@sympatico.ca,
> pgoswami@quickclic.net
>
>
> *
> Tubes with embedded aluminum fins or hot-dip galvanized steel fins,
> applicable up to a maximum operating temperature of 360 °C, should be used.
> Hot-dip galvanised steel fins shall not be used on austenitic steel tubing.
>
>
>
> *
>
>
> -----Original Message-----
> From: materials-welding@googlegroups.com
> [mailto:materials-welding@googlegroups.com] On Behalf Of Priya Deshmukh
> Sent: Saturday, December 24, 2011 1:24 AM
> To: materials-welding
> Subject: [MW:13288] To increase hardness of Heat Exchanger fin
>
> To,
>
> All.
>
> Please provide me the procedure to increase the hardness of fin material
> without affecting its thermal conductivity.
>
> May be some spray or liquid may be available, by spraying or dipping the
> fins into the liquid the hardness can be increased.
>
> Thanks,
>
> --
> Priyanka Deshmukh
>
> --
> To post to this group, send email to materials-welding@googlegroups.com
> To unsubscribe from this group, send email to
> materials-welding+unsubscribe@googlegroups.com
> For more options, visit this group's bolg at
> http://materials-welding.blogspot.com/
> The views expressed/exchnaged in this group are members personel views and
> meant for educational purposes only, Users must take their own decisions
> w.r.t. applicable code/standard/contract documents.
>
>
> --
> To post to this group, send email to materials-welding@googlegroups.com
> To unsubscribe from this group, send email to
> materials-welding+unsubscribe@googlegroups.com
> For more options, visit this group's bolg at
> http://materials-welding.blogspot.com/
> The views expressed/exchnaged in this group are members personel views and
> meant for educational purposes only, Users must take their own decisions
> w.r.t. applicable code/standard/contract documents.
>

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.



--
regards,
Harish.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

Comments

Popular posts from this blog

Materails FAQs

Q: What are equivalents for standard Q 235 B (and Q 235 A) for U-channels? (asked by: boris.vielhaber@vait.com) A: DIN Nr. = 2393 T.2, 2394 T.2, EN 10025 W. Nr. DIN 17007 = 1.0038 Design DIN 17006 = RSt 37-2, S235JRG2 (Fe 360 B) Q: What is St DIN 2391 BK material? (asked by: dmcandrews@automaticstamp.com) A: Precision steel tubes, cold-finished/hard. Q: What is C.D.W. Boiler Tube? (asked by: montydude123@yahoo.com) A: Cold Drawn Welded Boiler Tube. Q: WHAT IS W.Nr. 1.4301? PLS TELL US IN EASY LANGUAGUE (asked...

[MW:36169] Cold Bending Qualification

Dear Experts,  Can anyone share the inspection requirements or a qualification procedure for cold bending? Our client spec states only the requirements for induction bending and would like to know your opinion on the cold bend inspection requirements. The code of construction is B31.3, Max. 5D bends, A106 SS 316L.  Thanks in Advance. -- https://materials-welding.blogspot.com/ https://www.linkedin.com/groups/122787 --- You received this message because you are subscribed to the Google Groups "Materials & Welding" group. To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com . To view this discussion visit https://groups.google.com/d/msgid/materials-welding/1be61cc3-e9c9-4a5f-834d-e8485e248432n%40googlegroups.com .

Heat tint (temper) colours on stainless steel surfaces heated in air // Heat tint

Introduction The colour formed when stainless steel is heated, either in a furnace application or in the heat affected zone of welds, is dependent on several factors that are related to the oxidation resistance of the steel. The heat tint or temper colour formed is caused by the progressive thickening of the surface oxide layer and so, as temperature is increased, the colours change.   Oxidation resistance of stainless steels However, there are several factors that affect the degree of colour change and so there is no a single table of colour and temperature that represents all cases. The colours formed can only be used as an indication of the temperature to which the steel has been heated. Factors affecting the heat tint colours formed Steel composition The chromium content is the most important single factor affecting oxidation resistance. The higher the chromium, the more heat resistant the steel and so the development of the heat tint colou...