Skip to main content

Re: [MW:13262] Identification of thickness on Radiography films.

Dear Vichare..

  as per ASME SEC V article 2, the manufacturer shall include the minimum radiographic parameters in the radiography documentation, so as per sec V it has not been mentioned the thickness had to be included in the radiography film identification but it has to be included in documentation(report). kindly look at the the qualified procedure for any such classes for the film identification. if it is in a single report if there are different thickness joints, u can ask them to add the thickness in the radiography report against each joint, or u can ask them to make a single report for each thickness so it will be easy for the interpreter to view the IQI requirements..

Regards 
Raju Kandula

On Thu, Dec 22, 2011 at 2:59 PM, Ramchandra vichare <vicharerke@indiatimes.com> wrote:
Dear Experts,

During Interpreting Radiography films at one of my vendor's works, I observed that, there is no identification /indicate thickness of job on film so I rejected the film. As far as generally everyone related field experience persons are know unless identification of thickness on film it is very difficult to know which penetrameter to be used but my vendor is arguing for the same. According to him one of "Level III" person insisit them there is no need to mentioned thickness in Radiography films and it sufficient if it indicate in Radiography interpretion report.
Suppose in piping number of joints/piping spools  are comming  with verious thickness in same report in such case it is possible to identify required penetrameter ? My anser is no, each Radiography films must be indicat thickness of joint/job.  Requested to suggest/advise.

Sincerely yours,
RK Vichare

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

Comments

Popular posts from this blog

Materails FAQs

Q: What are equivalents for standard Q 235 B (and Q 235 A) for U-channels? (asked by: boris.vielhaber@vait.com) A: DIN Nr. = 2393 T.2, 2394 T.2, EN 10025 W. Nr. DIN 17007 = 1.0038 Design DIN 17006 = RSt 37-2, S235JRG2 (Fe 360 B) Q: What is St DIN 2391 BK material? (asked by: dmcandrews@automaticstamp.com) A: Precision steel tubes, cold-finished/hard. Q: What is C.D.W. Boiler Tube? (asked by: montydude123@yahoo.com) A: Cold Drawn Welded Boiler Tube. Q: WHAT IS W.Nr. 1.4301? PLS TELL US IN EASY LANGUAGUE (asked...

[MW:30043] Weep hole

If weep hole is not provided in dummy pipe before welding What will happen??? -- https://materials-welding.blogspot.com/ https://www.linkedin.com/groups/122787 --- You received this message because you are subscribed to the Google Groups "Materials & Welding" group. To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com . To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/da251ee6-fa7f-4851-b876-cdb3834ae341%40googlegroups.com .

[MW:36169] Cold Bending Qualification

Dear Experts,  Can anyone share the inspection requirements or a qualification procedure for cold bending? Our client spec states only the requirements for induction bending and would like to know your opinion on the cold bend inspection requirements. The code of construction is B31.3, Max. 5D bends, A106 SS 316L.  Thanks in Advance. -- https://materials-welding.blogspot.com/ https://www.linkedin.com/groups/122787 --- You received this message because you are subscribed to the Google Groups "Materials & Welding" group. To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com . To view this discussion visit https://groups.google.com/d/msgid/materials-welding/1be61cc3-e9c9-4a5f-834d-e8485e248432n%40googlegroups.com .