Re: [MW:13251] Tandem MIG welding

Reduce the current and use mixer of 80Ar+18Co2+2O2

On 12/20/11, Paresh Katvi <pkatvi@gmail.com> wrote:
> Please control your travel speed of Job and try to do fore hand technique.
> Regards
> PRK
>
> On 12/18/11, S C Balawat <scb12345@gmail.com> wrote:
>>
>> Good morning group members ,
>>
>> I would like to know your experience in Mig welding with TBi TD 20 Tandem
>> torch of TBI industries . We are experiencing problems like burn through,
>> excessive spatters, undercut in the welds. Weld is fillet of 10 mm. We
>> simultaneously weld two fillets using robots. Job rotates in vertical
>> plane
>> and the robots are stationary . We are unable to stabilize the weld
>> quality
>> . Thickness of the at the joint is 10 mm and 14 mm in one weld joint and
>> in
>> another it is 10 mm and 12 mm.Welding gas is 90/10 argon / CO2.Power
>> source
>> is "power wave robotic 655 " of Lincoln Electric
>>
>> We are using 1.6 mm solid wire in the leading torch and 1.2 mm in the
>> following torch . Weld parameters are 400amps/28 volts and 360amps /27
>> volts
>> respectively.weld wire is ER70S-6 in Marathon spools. Weld wire is ESSAB
>> make .Material of the joint members is AISI 1020.
>>
>> I look forward to your comments /suggestions.
>>
>> Regards,
>>
>> S C Balawat
>>
>>
>> Sent from my iPad
>>
>> --
>> To post to this group, send email to materials-welding@googlegroups.com
>> To unsubscribe from this group, send email to
>> materials-welding+unsubscribe@googlegroups.com
>> For more options, visit this group's bolg at
>> http://materials-welding.blogspot.com/
>> The views expressed/exchnaged in this group are members personel views and
>> meant for educational purposes only, Users must take their own decisions
>> w.r.t. applicable code/standard/contract documents.
>>
>
> --
> To post to this group, send email to materials-welding@googlegroups.com
> To unsubscribe from this group, send email to
> materials-welding+unsubscribe@googlegroups.com
> For more options, visit this group's bolg at
> http://materials-welding.blogspot.com/
> The views expressed/exchnaged in this group are members personel views and
> meant for educational purposes only, Users must take their own decisions
> w.r.t. applicable code/standard/contract documents.
>

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

Comments

Popular posts from this blog

Heat tint (temper) colours on stainless steel surfaces heated in air // Heat tint

Introduction The colour formed when stainless steel is heated, either in a furnace application or in the heat affected zone of welds, is dependent on several factors that are related to the oxidation resistance of the steel. The heat tint or temper colour formed is caused by the progressive thickening of the surface oxide layer and so, as temperature is increased, the colours change.   Oxidation resistance of stainless steels However, there are several factors that affect the degree of colour change and so there is no a single table of colour and temperature that represents all cases. The colours formed can only be used as an indication of the temperature to which the steel has been heated. Factors affecting the heat tint colours formed Steel composition The chromium content is the most important single factor affecting oxidation resistance. The higher the chromium, the more heat resistant the steel and so the development of the heat tint colou...

[MW:5202] RE: 5200] NDT after PWHT

------------------------------------- Interpretation:  I‑89‑14 Subject:         Section I (1986 Edition, 1987 Addenda), PW‑11,                  NDE Prior to PWHT Date Issued:     December 15, 1988 File:            BC88‑393   Question: Does PW‑11 require that NDE be performed on welds after they have been subjected to the postweld heat treatment required by PW‑39?   Reply: No, unless the conditions described in PW‑11.2.2 exist. ---------------------------------------------- Interpretation:  VIII-1-98-09 Subject:         Section VIII, Division 1 (1995 Edition, 1996 Addenda); NDE                 ...

Materails FAQs

Q: What are equivalents for standard Q 235 B (and Q 235 A) for U-channels? (asked by: boris.vielhaber@vait.com) A: DIN Nr. = 2393 T.2, 2394 T.2, EN 10025 W. Nr. DIN 17007 = 1.0038 Design DIN 17006 = RSt 37-2, S235JRG2 (Fe 360 B) Q: What is St DIN 2391 BK material? (asked by: dmcandrews@automaticstamp.com) A: Precision steel tubes, cold-finished/hard. Q: What is C.D.W. Boiler Tube? (asked by: montydude123@yahoo.com) A: Cold Drawn Welded Boiler Tube. Q: WHAT IS W.Nr. 1.4301? PLS TELL US IN EASY LANGUAGUE (asked...