Re: [MW:13250] Technical Query for MIXER / ASME B 31.3 Vs ASME Sec VIII Div 1

Though according to ASME B31.3, it falls under Category M Fluid service for which if P1 material PWHT exempted upto 20mm as per Table 331.1.1 but if client is particular then it is advisable to do PWHT.
 
Thanks & Reagrds
 
J.Gerald Jayakumar
00968-93281596
From: Vino Varghese <vinopvarghese@gmail.com>
To: materials-welding@googlegroups.com
Cc: Vinop Varughese <vinop.varughese@qcon.com.qa>
Sent: Wednesday, December 21, 2011 3:21 PM
Subject: [MW:13247] Technical Query for MIXER / ASME B 31.3 Vs ASME Sec VIII Div 1

Dear Experts,
 
We have a Piping Component, named MIXER(Sour Service & Lethal) which is coming in line with Pipeline.
 
1. The Data Sheet of this Mixer refers to Calculation part as per ASME Sec VIII, Div 1 , 2010 Ed.
2. The fabrication, inspection, testing refers to ASME B 31.3.
 
Query: Client is requesting to do Post Weld Heat Treatment for all the Weld joints as service is Lethal(UW-2 of ASME Sec VIII, Div 1 ).
 
We tried to convince Client stating that this requirement of PWHT is not required as per ASME B 31.3 as this is not a Pressure Component(U-1(c)(2)(e), ASME Sec VIII, Div 1) and moreover, only the Calculation part of MIXER has been considered in accordance to ASME Sec VIII, Div 1.
Client still insisit for PWHT of all related weld joints as the Process stream of this mixer has been considered "LETHAL", hence it is applicable to MIXER too. The MIXER is completed, painted and recieved at our end from Supplier without PWHT.
 
Please provide your technical support to justify the Query and what further appropriate action can be considered.
 
Thanks & Regards
Vino P Varghese
Doha- Qatar
 
 
 
 
 
 
 
--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.


Comments

Popular posts from this blog

Materails FAQs

Q: What are equivalents for standard Q 235 B (and Q 235 A) for U-channels? (asked by: boris.vielhaber@vait.com) A: DIN Nr. = 2393 T.2, 2394 T.2, EN 10025 W. Nr. DIN 17007 = 1.0038 Design DIN 17006 = RSt 37-2, S235JRG2 (Fe 360 B) Q: What is St DIN 2391 BK material? (asked by: dmcandrews@automaticstamp.com) A: Precision steel tubes, cold-finished/hard. Q: What is C.D.W. Boiler Tube? (asked by: montydude123@yahoo.com) A: Cold Drawn Welded Boiler Tube. Q: WHAT IS W.Nr. 1.4301? PLS TELL US IN EASY LANGUAGUE (asked...

[MW:36169] Cold Bending Qualification

Dear Experts,  Can anyone share the inspection requirements or a qualification procedure for cold bending? Our client spec states only the requirements for induction bending and would like to know your opinion on the cold bend inspection requirements. The code of construction is B31.3, Max. 5D bends, A106 SS 316L.  Thanks in Advance. -- https://materials-welding.blogspot.com/ https://www.linkedin.com/groups/122787 --- You received this message because you are subscribed to the Google Groups "Materials & Welding" group. To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com . To view this discussion visit https://groups.google.com/d/msgid/materials-welding/1be61cc3-e9c9-4a5f-834d-e8485e248432n%40googlegroups.com .

Heat tint (temper) colours on stainless steel surfaces heated in air // Heat tint

Introduction The colour formed when stainless steel is heated, either in a furnace application or in the heat affected zone of welds, is dependent on several factors that are related to the oxidation resistance of the steel. The heat tint or temper colour formed is caused by the progressive thickening of the surface oxide layer and so, as temperature is increased, the colours change.   Oxidation resistance of stainless steels However, there are several factors that affect the degree of colour change and so there is no a single table of colour and temperature that represents all cases. The colours formed can only be used as an indication of the temperature to which the steel has been heated. Factors affecting the heat tint colours formed Steel composition The chromium content is the most important single factor affecting oxidation resistance. The higher the chromium, the more heat resistant the steel and so the development of the heat tint colou...