RE: [MW:13350] RE: 13271] Technical Query for MIXER / ASME B 31.3 Vs ASME Sec VIII Div 1

Hi Vino

 

Combining of two codes are not regular practice, however, the owner, depends upon the service criteria may select combination of Codes or his specifications if he wishes.

 

However, when there is a Code stamping requirement like U-stamp, the complete design, construction, inspection and testing shall meet the minimum requirements of respective Codes. There are many client, who provides amendments to the Codes are more restrictive than Codes.

 

In this case, the selection of Sec VIII may not be appropriate since, the item mixer is exempted from Sec VIII and due to design input / output (piping stress analysis, thermal expansion/contraction, pipe supports are different from Sec VIII). Refer to my email below as stated earlier.

 

But as per Codes perspective, No Code allows the use of multiple Code for the single construction unless it is stated so, however the Client is always BOSS. If there is any conflict, it is better to resolve it in advance.

 

You are really lucky that you got accepted but many clients….? (needs the same broken pot)!!!

Cheers

BR

M.Vijayan

 

From: materials-welding@googlegroups.com [mailto:materials-welding@googlegroups.com] On Behalf Of Vino Varghese
Sent: Monday, December 26, 2011 9:01 PM
To: materials-welding@googlegroups.com
Subject: Re: [MW:13319] RE: 13271] Technical Query for MIXER / ASME B 31.3 Vs ASME Sec VIII Div 1

 

Dear Vijay,

 

I totally agree with regard to Vessel if fabricated in accordance to ASME Section VIII, Div 1.

Here the Mixer should have been fabricated as per ASME B31.3 because the Data sheet refer to Calculation part as ASME SEC VIII, Div 1 and fabrication as per Piping Class...

 

Client now got convienced and request the Data sheet to revise to show Calculation as ASME B 31.3 and "LETHAL" Service can be avoided.

 

Query: Can we have only the calculation as per ASME Sec VIII Div 1 and all fabrication, Inspection and other requirements as per ASME B 31.3? Whether this is a Acceptable Practice.

 

Throw some more light....

 

Regards

VPV

 

__________________________________________________________________________________



 

On Sun, Dec 25, 2011 at 11:17 AM, vijayan <vijayan.m@madinagulf.com> wrote:

Hi Vino

 

PWHT is Reqd for the below reasons.

 

-// We tried to convince Client stating that this requirement of PWHT is not required as per ASME B 31.3 as this is not a Pressure Component(U-1(c)(2)(e), ASME Sec VIII, Div 1) //

 

Refer U-1(d). from the interpretation of the clause; any vessel/part can be designed to ASME Sec VIII and still can be stamped. This requirement is generally dictated by Client. It is the Client responsibility to dictate the service requirements. Here client has specified you the service as “Lethal” (refer U-2)

 

Refer UW-2 Service restrictions (excerpt)

…. If determined as lethal, the user and / or his designated agent [see U-2(a)] shall so advise the designer and / or manufacturer. It shall be the responsibility of the manufacturer to comply with the applicable Code provisions (see UCI-2 and UCD-2)

 

// only the Calculation part of MIXER has been considered in accordance to ASME Sec VIII, Div 1.//

 

The design Calculations derived from UG and as well as applicable UW for design calculations such as applicable joint type, Joint efficiency, requirement of NDT based on joint efficiency. (refer UG-16)

 

Extract from B 31.3

 

 

My Conclusion

The owner might have selected Category M fluid design requirements here, but specifically he selected ASME Sec VIII, Div.1 for the valid reasons he may have.

Moreover, the term “Lethal” is not addressed any where in the B 31.3 Code but it is very well addressed in ASME Sec VIII. So, the client very much aware of his design and related construction requirements. So as per my preseceptive, the item requires PWHT.

Othere seniors may throw some light

BR

M.Vijayan

 

From: materials-welding@googlegroups.com [mailto:materials-welding@googlegroups.com] On Behalf Of Vino Varghese
Sent: Thursday, December 22, 2011 11:12 PM
To: materials-welding@googlegroups.com
Subject: [MW:13271] Technical Query for MIXER / ASME B 31.3 Vs ASME Sec VIII Div 1

 

Dear Experts,

 

We have a Piping Component(Thickness 9.5mm), named MIXER(Sour Service & Lethal) which is coming in line with Pipeline.

 

1. The Data Sheet of this Mixer refers to Calculation part as per ASME Sec VIII, Div 1 , 2010 Ed.

2. The fabrication, inspection, testing refers to ASME B 31.3.

 

Query: Client is requesting to do Post Weld Heat Treatment for all the Weld joints as service is Lethal(UW-2 of ASME Sec VIII, Div 1 ).

 

We tried to convince Client stating that this requirement of PWHT is not required as per ASME B 31.3 as this is not a Pressure Component(U-1(c)(2)(e), ASME Sec VIII, Div 1) and moreover, only the Calculation part of MIXER has been considered in accordance to ASME Sec VIII, Div 1.

Client still insisit for PWHT of all related weld joints as the Process stream of this mixer has been considered "LETHAL", hence it is applicable to MIXER too. The MIXER is completed, painted and recieved at our end from Supplier without PWHT.

 

Please provide your technical support to justify the Query and what further appropriate action can be considered.

 

Thanks & Regards

Vino P Varghese

Doha- Qatar

 

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

 


This communication and any files transmitted with it are confidential and may also be privileged. It is for the exclusive use of the intended recipient(s). If you are not the intended recipient or the person responsible for delivering it to the intended recipient(s), please note that any form of distribution, copying or use of this communication or information contained in it is strictly prohibited and may be unlawful. If you have received this communication in error please return it to the sender, and delete the material from any computer. We reserve the right to monitor email communications through normal internal and external networks. We believe but not warrant that the email and the attachments are virus free. The statement and opinions expressed in this communication are those of the writer and do not necessarily represent those of Madina Group, whose registered office address is

P.O. Box 20459, Doha, Qatar.
Tel. +974 44600818
Fax. +974 44603143

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

 

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.



This communication and any files transmitted with it are confidential and may also be privileged. It is for the exclusive use of the intended recipient(s). If you are not the intended recipient or the person responsible for delivering it to the intended recipient(s), please note that any form of distribution, copying or use of this communication or information contained in it is strictly prohibited and may be unlawful. If you have received this communication in error please return it to the sender, and delete the material from any computer. We reserve the right to monitor email communications through normal internal and external networks. We believe but not warrant that the email and the attachments are virus free. The statement and opinions expressed in this communication are those of the writer and do not necessarily represent those of Madina Group, whose registered office address is

P.O. Box 20459, Doha, Qatar.
Tel. +974 44600818
Fax. +974 44603143

Comments

Popular posts from this blog

Materails FAQs

Q: What are equivalents for standard Q 235 B (and Q 235 A) for U-channels? (asked by: boris.vielhaber@vait.com) A: DIN Nr. = 2393 T.2, 2394 T.2, EN 10025 W. Nr. DIN 17007 = 1.0038 Design DIN 17006 = RSt 37-2, S235JRG2 (Fe 360 B) Q: What is St DIN 2391 BK material? (asked by: dmcandrews@automaticstamp.com) A: Precision steel tubes, cold-finished/hard. Q: What is C.D.W. Boiler Tube? (asked by: montydude123@yahoo.com) A: Cold Drawn Welded Boiler Tube. Q: WHAT IS W.Nr. 1.4301? PLS TELL US IN EASY LANGUAGUE (asked...

[MW:36169] Cold Bending Qualification

Dear Experts,  Can anyone share the inspection requirements or a qualification procedure for cold bending? Our client spec states only the requirements for induction bending and would like to know your opinion on the cold bend inspection requirements. The code of construction is B31.3, Max. 5D bends, A106 SS 316L.  Thanks in Advance. -- https://materials-welding.blogspot.com/ https://www.linkedin.com/groups/122787 --- You received this message because you are subscribed to the Google Groups "Materials & Welding" group. To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com . To view this discussion visit https://groups.google.com/d/msgid/materials-welding/1be61cc3-e9c9-4a5f-834d-e8485e248432n%40googlegroups.com .

Heat tint (temper) colours on stainless steel surfaces heated in air // Heat tint

Introduction The colour formed when stainless steel is heated, either in a furnace application or in the heat affected zone of welds, is dependent on several factors that are related to the oxidation resistance of the steel. The heat tint or temper colour formed is caused by the progressive thickening of the surface oxide layer and so, as temperature is increased, the colours change.   Oxidation resistance of stainless steels However, there are several factors that affect the degree of colour change and so there is no a single table of colour and temperature that represents all cases. The colours formed can only be used as an indication of the temperature to which the steel has been heated. Factors affecting the heat tint colours formed Steel composition The chromium content is the most important single factor affecting oxidation resistance. The higher the chromium, the more heat resistant the steel and so the development of the heat tint colou...