Dear Mr.Pieper

Thank you for your info.

Could you pl. give the units for measuring the surface roughness. As per my client spec. it is mentioned as microns only.

I think surface appearance after blasting should be SA 2 1/2 or SA 3 and should not be measured in microns.

thank you
Rao


From: Pieper QSI <info@pieper-qsi.nl>
To: materials-welding@googlegroups.com
Sent: Friday, 23 December 2011 2:07 PM
Subject: RE: [MW:13277] Surface roughness measurement instruments.

Dear Mr. Rao,
 
Be aware that the microns you mention is not the surface roughness but the coating layer thickness (DFT = Drie Film Thickness).
For surface roughness you will have values like SA 2,5 microns or similar and in practice mostly the comparators are used for inspection prior to first layer of coating.
After fist coating layer there is no need to measure the roughness anymore.
 
Met vriendelijke groeten / Best Regards
 
Herman Pieper
 
Pieper Quality Support & Inspection
Phone: +31 (0)521 380083
Fax:     +31 (0)84 7539225
Cell:     +31 (0)6 51691215
www.pieper-qsi.nl
 
Van: materials-welding@googlegroups.com [mailto:materials-welding@googlegroups.com] Namens jsrisud@gmail.com
Verzonden: donderdag 22 december 2011 14:45
Aan: materials-welding@googlegroups.com
Onderwerp: Re: [MW:13259] Surface roughness measurement instruments.
 
Dear Mr. Rao,

There are portable surface roughness measuring instruments to measure as required.

UK based Rank Taylor Hobson instruments are available in India.

Srinivasan
Sent from BlackBerry® on Airtel

From: Vasantharao <vasantharao@yahoo.in>
Date: Thu, 22 Dec 2011 15:38:40 +0530 (IST)
Subject: [MW:13256] Surface roughness measurement instruments.
 
Dear Experts,
 
I work as inspection Engineer. When i go for Blasting inspection, contractor provided  me profile comparator for surface roughness measurement.
 
Contractor do  Grit blasting in the shop.
 
I need to measure surface roughness  -  75-100 microns      Painting system No#1
                                                            50-75 microns        Painting system No#2

Queries
Q 1: Comparator is enough for surface roughness measurements.
 
Q2: Is any other tools available for roughness measurement?.
 
Q3:  What is the normal industry practice.


Pl. provide your valuable suggestions as i'm new for painting activities.

Rao.
 
--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.


Comments

Popular posts from this blog

Materails FAQs

Q: What are equivalents for standard Q 235 B (and Q 235 A) for U-channels? (asked by: boris.vielhaber@vait.com) A: DIN Nr. = 2393 T.2, 2394 T.2, EN 10025 W. Nr. DIN 17007 = 1.0038 Design DIN 17006 = RSt 37-2, S235JRG2 (Fe 360 B) Q: What is St DIN 2391 BK material? (asked by: dmcandrews@automaticstamp.com) A: Precision steel tubes, cold-finished/hard. Q: What is C.D.W. Boiler Tube? (asked by: montydude123@yahoo.com) A: Cold Drawn Welded Boiler Tube. Q: WHAT IS W.Nr. 1.4301? PLS TELL US IN EASY LANGUAGUE (asked...

[MW:36169] Cold Bending Qualification

Dear Experts,  Can anyone share the inspection requirements or a qualification procedure for cold bending? Our client spec states only the requirements for induction bending and would like to know your opinion on the cold bend inspection requirements. The code of construction is B31.3, Max. 5D bends, A106 SS 316L.  Thanks in Advance. -- https://materials-welding.blogspot.com/ https://www.linkedin.com/groups/122787 --- You received this message because you are subscribed to the Google Groups "Materials & Welding" group. To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com . To view this discussion visit https://groups.google.com/d/msgid/materials-welding/1be61cc3-e9c9-4a5f-834d-e8485e248432n%40googlegroups.com .

Heat tint (temper) colours on stainless steel surfaces heated in air // Heat tint

Introduction The colour formed when stainless steel is heated, either in a furnace application or in the heat affected zone of welds, is dependent on several factors that are related to the oxidation resistance of the steel. The heat tint or temper colour formed is caused by the progressive thickening of the surface oxide layer and so, as temperature is increased, the colours change.   Oxidation resistance of stainless steels However, there are several factors that affect the degree of colour change and so there is no a single table of colour and temperature that represents all cases. The colours formed can only be used as an indication of the temperature to which the steel has been heated. Factors affecting the heat tint colours formed Steel composition The chromium content is the most important single factor affecting oxidation resistance. The higher the chromium, the more heat resistant the steel and so the development of the heat tint colou...