Re: [MW:12587] Normalizing of dished end

Dear Vishal

First of ASME SEC VIII DIV-1 does not ask for Normalizing of forming part.

In your case, Even  Code does not ask for PWHT also.

Even if  PWHT is required as per UCL-34, code specify the same with caution notes as below

Postweld heat treatment may be in the carbide-precipitation range for unstabilized austenitic chromium–nickel steels, as well as within the range where a sigma phase may form, and if used indiscriminately could result in material of inferior physical properties and inferior corrosion resistance, which ultimately could result in failure of the vessel.

Hence in your case normalishing is neither recommended nor required.
Best Regards

Rajesh Patel
Executive Engineer  - Materials Technology, QA/QC & Standards





From:        VIshal Sapkale <sapkalevishalv@gmail.com>
To:        materials-welding@googlegroups.com
Date:        30.09.11 05:52
Subject:        [MW:12583] Normalizing of dished end
Sent by:        materials-welding@googlegroups.com






--
Dear Experts,

We have Clad plate (SA516 Gr.70 thk 18mm +SA 240 TP 316L thk.4mm). We formed dished end from that plate. normally we do normalizing for the thk above 16mm dish.
so can anyone tell me whether we can normalize the dished endof thk 18+4mm.
If yes then why? and if not, why?






Regards,
Vishal

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at
http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...