Re: [MW:12560] PWHT Requirement for SA 335 P91 (or P no. 5B Group 2/ 15E group 1)

@Raghuram ... Thank you very much for your prompt and sufficient response
@Goswami Sir! Please see the table below. If you require more information i will forward 


Regards
ASIF
+971-50-9198730
On Tue, Sep 27, 2011 at 4:00 PM, pgoswami <pgoswami@quickclic.net> wrote:
Hello Asif,
 
I have seen the use of P-91 material in conventional thermal generation units, coal, HRSG ,Coal+Biomass. If the plant in question is a solar power plant, then what're the design and operating conditions (e.g temperature, pressure )?
 
Appreciate your response. 
 
Thanks.
 
Pradip Goswami,P.Eng.IWE
Welding & Metallurgical Specialist & Consultant
Ontario,Canada.
Email-pgoswami@sympatico.ca,
 


From: materials-welding@googlegroups.com [mailto:materials-welding@googlegroups.com] On Behalf Of Bathula Raghuram (Mumbai - PIPING)
Sent: Tuesday, September 27, 2011 1:30 AMSubject: RE: [MW:12546] PWHT Requirement for SA 335 P91 (or P no. 5B Group 2/ 15E group 1)

It is included in B31.1 as P5B in old editions, however  this material is regrouped as P15E in latest edition of ASME BPV Sec IX, , pl refer the table below.

 

From: materials-welding@googlegroups.com [mailto:materials-welding@googlegroups.com] On Behalf Of ASIF
Sent: Tuesday, September 27, 2011 10:42 AM
To: materials-welding@googlegroups.com
Subject: [MW:12545] PWHT Requirement for SA 335 P91 (or P no. 5B Group 2)

 


Dear experts!

 

 

Project : Solar Power Plant

Construction Code ASME B31.1

 

ASME Sec IX

 

PWHT Requirement - SA 335 P91 or P no. 5B Group 2 material is not included in 132 Para and Table of B31.1, and also,

ASME Sec IX para QW-407 do not mention this material group.

 

Client Specification do not mention this requirement separately

 

Please advise! do we need to go for PWHT ?

 

 


--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.






--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

[MW:35692]

Dear all    Can I do MPI above painting surface for cs  tank  Regards, Sriram Srinivasan -- https://materials-welding.blog...