Re: [MW:12533] spot radiography as per ASME B 31.3

Dear Azhar,
Spot Radiography is to be taken on joint but random examination is be selected from the lot.
 
Thanks & Regards,
Mohd.Azam

On Mon, Sep 26, 2011 at 8:47 AM, Azhar Ali <aab51214@yahoo.com> wrote:
DEAR EXPERTS

let me know the extent of radiography as per ASME B31.3 for normal service.

Can any body elaborate the the difference between spot and random examination as per para no.344.1.3. 


Regards

Azhar Ali


--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

[MW:35692]

Dear all    Can I do MPI above painting surface for cs  tank  Regards, Sriram Srinivasan -- https://materials-welding.blog...