Dear Sir,


Normally E 7010 is suitable for root welding as it will give good penetration. Hot pass fill up you may use E7018. When PQR required impact test your electrode shall be impact  tested higher than the required temperature. It is only assumption as you have not given the base metal quality grade etc.






Thanking You,

Honesty is the best Policy

With Warm Regards,

Muthu Barathi P
Mobile No:00962788269821 (Jordan)
00962775401951


From: sevak hiren <hirensevak80@gmail.com>
Sent: Mon, 26 Sep 2011 09:25:44
To: materials-welding@googlegroups.com
Subject: Re: [MW:12524] PQR by E7010 4mm electrode
You are not clear..

Which electride you used for root run ?

What is the job thk ?

What was the root gap ?

I suggest use GTAW root & E 7018 fill.

On 9/25/11, mpk mpk <ranmi2007@gmail.com> wrote:
> Dear Experts,
>
> We have carried out PQR by E7010 4mm electrode for fill passes but it was
> unsuccessful in root bend test.We have carried out same process in repair
> PQR which is successful.
>
> So plz give me your advice which will help me in next PQR.
>
> Thank you...
> MPK
>
> --
> To post to this group, send email to materials-welding@googlegroups.com
> To unsubscribe from this group, send email to
> materials-welding+unsubscribe@googlegroups.com
> For more options, visit this group's bolg at
> http://materials-welding.blogspot.com/
> The views expressed/exchnaged in this group are members personel views and
> meant for educational purposes only, Users must take their own decisions
> w.r.t. applicable code/standard/contract documents.
>


--
Thanks & Regards

Hiren Sevak
Surveyor
Bureau Veritas - Ahmedabad
207, Abhishree
Opp Star India Bazaar,
Satellite Road,
Ahmedabad-380015
Tel No. 079-26925491/92

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.


Treat yourself at a restaurant, spa, resort and much more with Rediff Deal ho jaye!

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

[MW:35692]

Dear all    Can I do MPI above painting surface for cs  tank  Regards, Sriram Srinivasan -- https://materials-welding.blog...