Re: [MW:12530] GTAW/SMAW which process is high Heat Input.

Dear MKP,

The power at the ARC GAP in 

GTAW = Welding Current * [10 + 0.04x Welding Current]
SMAW = Welding Current * [20 + 0.04x Welding Current] 

So even at the same current level the heat input for SMAW is more than that in GMAW, plus with additional features like Pulsed GTAW, it is easier to reduce the heat input (the same option is not possible in SMAW).

Regards,

Nimesh S Chinoy
SigmaWeld

On Mon, Sep 26, 2011 at 8:21 AM, mpk mpk <ranmi2007@gmail.com> wrote:
Dear Experts,
 
GTAW/SMAW which process is high Heat Input.
 
Thank you
MPK

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.



--
Nimesh S Chinoy

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...