Thursday, September 22, 2011

Re: [MW:12503] SS 316 L VESSEL HYDROTEST WATER QUALITY

Hello Mr.Lassaad,
 
Find the below requirement from Saudi Aramco Material System Spec 32-SAMSS-004 for your query...
 

16.3.9     Water used for pressure testing shall be potable.  For vessels manufactured from stainless steel, the water shall not contain more than 50 ppm chlorides with pH value of 10 to 11 at the time of filling the vessel.

16.3.10   The temperature of the water during hydrostatic testing shall be maintained at not less than 17°C throughout the testing cycle.

I think this will help you...

On Wed, Sep 21, 2011 at 1:21 PM, lassaad mokrani <lassaad.mokrani@gmail.com> wrote:
Dear Experts,
Could you inform me if there an obligation in ASME IIIV Div 1, about the quality of hydrotest water.
Our 2 vessels are in SS 316L with operating temperatures respectively 21°C and -5°C

Best Regards,


--
Meilleures salutations

Mokrani Lassaad
00216 20 649 755
http://www.linkedin.com/pub/lassaad-mokrani/16/364/907


















P     Pensez environnement! N'imprimez ce mail que si c'est vraiment nécessaire
Please consider your environmental responsibility before printing this e-mail


This e-mail is confidential and it is intended only for the addressees. Any
review, dissemination, distribution, or copying of this message by persons
or entities other than the intended recipient is prohibited. If you have
received this e-mail in error, kindly notify us immediately by telephone or
e-mail and delete the message from your system. The sender does not accept
liability for any errors or omissions in the contents of this message which
may arise as a result of the e-mail transmission

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.



--
G.Murali krishnan

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

[MW:35692]

Dear all    Can I do MPI above painting surface for cs  tank  Regards, Sriram Srinivasan -- https://materials-welding.blog...