Thursday, September 22, 2011

Re: [MW:12502] WELD DEFECT:-BURN THROUGH IN SAW WELDING IS ACCEPTABLE FOR PSL2 PIPES

Hi Mohammad,

You are correct to say that nothing is mentioned in API 5L spec but Arc burns are not acceptable by spec so i treat Burn through in similar manner,

Removal and rewelding would be required so you should have a Weld repair PQR to do the repairs, if not then qualify a new PQR (if intending to use process other than SAW), check client spec to know if any additional requirement for the repairs (PWHT etc...)

Should you need any info feel free to post.

Regards
Manpreet Singh



Sent: Sun, 18 Sep 2011 16:58:32 +0530 (IST)

Subject: [MW:12477] WELD DEFECT:-BURN THROUGH IN SAW WELDING IS ACCEPTABLE FOR PSL2 PIPES



DEAR ALL


             NOTHING IS MENTIONED ABOUT WELD DEFECTS BURN THROUGH IN API 5L 44TH ADDITION FOR PSL2 PIPES.


 


I WANT TO NO IF BURN THROUGH DEFECTS COME BY SAW WELDING IT IS ACCEPTABLE OR REJECTABLE FOR PSL2 PIPES.


 


REGARDS


MOHAMMAD SAJID ALAM


INSPECTION ENGINEER


AICO-DAMMAM


MOBILE:-0534077860








--


To post to this group, send email to materials-welding@googlegroups.com


To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com


For more options, visit this group's bolg at http://materials-welding.blogspot.com/


The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.


Treat yourself at a restaurant, spa, resort and much more with Rediff Deal ho jaye!

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...