Re: [MW:12493] ASME SEC IX Code Issue

Dear Limesh

As per ASME Sec IX , Pre heat is essential variable not supplementary essential variable hence it is mandatory to observe the requirement of QW406.1

Inter pass temperature is supplementary requirement. However it is not applicable if PWHT performed above upper transformation temp i.e Normalizing, solution annealing as per QW 406.3

Hence in your case It doesn't give exemption to the requirement for Inter pass temperature


Best Regards

Rajesh Patel
Executive Engineer  - Materials Technology, QA/QC & Standards

Linde Engineering India Pvt. Ltd.
'Linde House'
Opp: VUDA Office,VIP Road, Karelibaug,Vadodara - 390018,India.
Tel.: +91 265 3056706, Fax: +91 265 23335213, Mobil: +91 9909953459
Rajesh.Patel@linde-le.com,
www.linde-india.com

This e-mail is confidential. If you are not the intended recipient, please notify us immediately. You should not disclose its contents to any other person nor use it for any purposes.




From:        usman gani <usmangania123@gmail.com>
To:        materials-welding@googlegroups.com
Date:        21-09-2011 15:25
Subject:        Re: [MW:12491] ASME SEC IX Code Issue
Sent by:        materials-welding@googlegroups.com




On 9/16/10, george.dilintas@gr.bureauveritas.com
<george.dilintas@gr.bureauveritas.com> wrote:
> According to ASME IX, QW-406.3, when the Preheat is a supplementary
> essential variable, an increase of more than 55 degC in the max Interpass
> temperature requires requalification.
> I would suggest you read carefully QW 406.1 to  406.3
>
> Dr. G. Dilintas - Authorized Inspector Supervisor
> I&F Regional Technical Manager
> Bureau Veritas Piraeus - Greece
> Tel: +30 210 40 63 113/4
> Fax: +30 210 40 63 118
> Cell: +30 69 44 64 62 04
>
>
>
>              limesh M
>              <limesh78@gmail.c
>              om>                                                        To
>              Sent by:                  materials-welding@googlegroups.com
>              materials-welding                                          cc
>              @googlegroups.com
>                                                                    Subject
>                                        [MW:6999] ASME SEC IX Code Issue
>              14/09/2010 15:43                                          Ref
>
>
>              Please respond to
>              materials-welding
>              @googlegroups.com
>
>
>
>
>
>
> Dear All,
> Design Code: ASME B31.3     Welding Code: ASME SEC IX
> I have a Low temperature carbon steel impact tested PQR with a PWHT range
> of 600⁰±10⁰C.Is this condition giving an exemption for me on QW406.3 to
> prepare a WPS with maximum interpass temperature of 200⁰C.
> Maximum interpass temperature observed during specimen welding: 140⁰C
>
> Regards,
>
> Limesh
>
>
> --
> To post to this group, send email to materials-welding@googlegroups.com
> To unsubscribe from this group, send email to
> materials-welding-unsubscribe@googlegroups.com
> For more options, visit this group's bolg at
>
http://materials-welding.blogspot.com/
> The views expressed/exchnaged in this group are members personel views and
> meant for educational purposes only, Users must take their own decisions
> w.r.t. applicable code/standard/contract documents.
>
> --
> To post to this group, send email to materials-welding@googlegroups.com
> To unsubscribe from this group, send email to
> materials-welding-unsubscribe@googlegroups.com
> For more options, visit this group's bolg at
>
http://materials-welding.blogspot.com/
> The views expressed/exchnaged in this group are members personel views and
> meant for educational purposes only, Users must take their own decisions
> w.r.t. applicable code/standard/contract documents.
>

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at
http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...