On 9/16/10, george.dilintas@gr.bureauveritas.com
<george.dilintas@gr.bureauveritas.com> wrote:
> According to ASME IX, QW-406.3, when the Preheat is a supplementary
> essential variable, an increase of more than 55 degC in the max Interpass
> temperature requires requalification.
> I would suggest you read carefully QW 406.1 to 406.3
>
> Dr. G. Dilintas - Authorized Inspector Supervisor
> I&F Regional Technical Manager
> Bureau Veritas Piraeus - Greece
> Tel: +30 210 40 63 113/4
> Fax: +30 210 40 63 118
> Cell: +30 69 44 64 62 04
>
>
>
> limesh M
> <limesh78@gmail.c
> om> To
> Sent by: materials-welding@googlegroups.com
> materials-welding cc
> @googlegroups.com
> Subject
> [MW:6999] ASME SEC IX Code Issue
> 14/09/2010 15:43 Ref
>
>
> Please respond to
> materials-welding
> @googlegroups.com
>
>
>
>
>
>
> Dear All,
> Design Code: ASME B31.3     Welding Code: ASME SEC IX
> I have a Low temperature carbon steel impact tested PQR with a PWHT range
> of 600⁰±10⁰C.Is this condition giving an exemption for me on QW406.3 to
> prepare a WPS with maximum interpass temperature of 200⁰C.
> Maximum interpass temperature observed during specimen welding: 140⁰C
>
> Regards,
>
> Limesh
>
>
> --
> To post to this group, send email to materials-welding@googlegroups.com
> To unsubscribe from this group, send email to
> materials-welding-unsubscribe@googlegroups.com
> For more options, visit this group's bolg at
> http://materials-welding.blogspot.com/
> The views expressed/exchnaged in this group are members personel views and
> meant for educational purposes only, Users must take their own decisions
> w.r.t. applicable code/standard/contract documents.
>
> --
> To post to this group, send email to materials-welding@googlegroups.com
> To unsubscribe from this group, send email to
> materials-welding-unsubscribe@googlegroups.com
> For more options, visit this group's bolg at
> http://materials-welding.blogspot.com/
> The views expressed/exchnaged in this group are members personel views and
> meant for educational purposes only, Users must take their own decisions
> w.r.t. applicable code/standard/contract documents.
>

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...