Friday, September 30, 2011

[MW:12590] CVN Impact test on 304L 2.77mm thick B31.3 piping

Please I need your assistance:-

I have Helium gas Pipeline 304L to be welded by ER308L ,having MDMT at
-269 Degree Centigrade , but the thickness of my Pipe is 2.77mm ,
Which is exempted from the impact requirements from B31.3 Chapter-III,
Table323.2.2 Column B, B-4, Notes -6, Impact test are not required
when maximum obtainable charpy specimen has a width along the notch of
less than 2.5mm.
but my client is not ready to accept that condition/constraint of
B31.3. he needs explanation that How the material thickness(2.5mm)
will bear that MDMT at -269 Degree Centigrad., even Obtainable charpy
specimen is not possible, but How to convince the client the material
will have the properties at that temperature.

Thanks & Regards
Posting on behalf of: Amit Pahuja

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

[MW:35692]

Dear all    Can I do MPI above painting surface for cs  tank  Regards, Sriram Srinivasan -- https://materials-welding.blog...