Friday, September 30, 2011

[MW:12589] Charpy Impact testing requirement for ASME B31.3 and API SPEC 6A welding application

Hello everyone,

I have a few questions that I need help with please:

1. When developing weld procedures to weld pipe materials like P1
(A106 grade A, B, C, and API 5L X-41, X-46, and X-56) to the same or
any P1 to P1 combination for ASME B31.3 application in an oil and gas
production site for flow lines, I do not need Charpy impact testing
for temperatures of -20F and above right?

2. What if I'm developing welding procedures to join API wellhead
flanges (materials: 4130 welded to the same), is there any minimum
temperature for Charpy impact requirement, in other words, if the
temperature anticipated is going to be -20F and above, is Charpy
impact testing required for this material. If Charpy is required and
it is not at -20F, at what temperature is it required, or do I have to
test for impact/toughness no matter what the temperature is for the
4130 material?

3. What if I'm developing a welding procedure to transition from API
wellhead to ANSI line pipe (material: 4130 to A106 B or any other P1
material), since the design of this joint is based on the weaker
material (A106 grade B or other applicable P1), do I need Charpy
impact testing for -20F and above?

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...