[MW:12583] Normalizing of dished end



--
Dear Experts,
We have Clad plate (SA516 Gr.70 thk 18mm +SA 240 TP 316L thk.4mm). We formed dished end from that plate. normally we do normalizing for the thk above 16mm dish.
so can anyone tell me whether we can normalize the dished endof thk 18+4mm.
If yes then why? and if not, why?






Regards,
Vishal

--