Skip to main content

Re: [MW:12287] Re: Difference between SB625 UNS NO8904 & SA 240 Type 904L

Dear Kapli,
As far I know,the UNS No. is unique for each material, it means that if one material introduced with one UNS No. and this material mentioned in two or more standards, they are the same.
 
Regards

On Sat, Aug 20, 2011 at 11:05 AM, kapil bhamburdekar <kapilbhamburdekar@gmail.com> wrote:
Dear Sir,

Thanks for your reply but i want to let you know that we have recieved
plate of SA 240 Type 904L, but as per our drawing it is to be SB625
UNS NO8904, so my question is after check testing of 904L plate is it
possible to recertify it to SB625 UNS NO8904 plate.

Assuming,All dimensional tolerances are satisfacory for 904L plate as
per SB625 UNS NO8904.

Regards,

Kapil

On Aug 19, 2:38 pm, meisam shokri arfaei <meisamsho...@gmail.com>
wrote:
> Dear Kapil,
> The uns N08904 is introdused in those two standards are the same (SA240
> TP904L and SB625 UNS N08904), but just in chemical and mechanical
> properties. There is too much restrictions in SB625 other than chemical and
> mechanical properties. If had a look on SB625 and it had some requirements
> for dimennsional and tolerances of products which theu are not mentioned in
> SA240.
>
> Regards
> On Fri, Aug 19, 2011 at 9:14 AM, kapil bhamburdekar <
>
>
>
>
>
> kapilbhamburde...@gmail.com> wrote:
> > Dear All Experts,
>
> > I want to know about the Difference between ASME SB625 UNS NO8904 & ASME SA
> > 240 Type 904L,
>
> > I have checked chemical and physical properties which are same for both,
> > but still Inspector is demanding for SB 625 Plate instead of ASME SA 240
> > Type 304 plate.
>
> > Regards,
>
> > Kapil Bhamburdekar
> > QA Engineer
>
> > --
> > To post to this group, send email to materials-welding@googlegroups.com
> > To unsubscribe from this group, send email to
> > materials-welding+unsubscribe@googlegroups.com
> > For more options, visit this group's bolg at
> >http://materials-welding.blogspot.com/
> > The views expressed/exchnaged in this group are members personel views and
> > meant for educational purposes only, Users must take their own decisions
> > w.r.t. applicable code/standard/contract documents.
>
> --
> M.Shokri Arfaei
> International Welding Engineer
> RT, UT ASNT Level III
> ERI-Metallurgy Lab. Manager
> Tel: +98 21 66283693
> Fax: +98 21 66283693
> Mob.: +98 912 139 4023
> Web:www.metallurgylab.com- Hide quoted text -
>
> - Show quoted text -

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.



--
M.Shokri Arfaei
International Welding Engineer
RT, UT ASNT Level III
ERI-Metallurgy Lab. Manager
Tel: +98 21 66283693
Fax: +98 21 66283693
Mob.: +98 912 139 4023
Web: www.metallurgylab.com

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

Comments

Popular posts from this blog

Materails FAQs

Q: What are equivalents for standard Q 235 B (and Q 235 A) for U-channels? (asked by: boris.vielhaber@vait.com) A: DIN Nr. = 2393 T.2, 2394 T.2, EN 10025 W. Nr. DIN 17007 = 1.0038 Design DIN 17006 = RSt 37-2, S235JRG2 (Fe 360 B) Q: What is St DIN 2391 BK material? (asked by: dmcandrews@automaticstamp.com) A: Precision steel tubes, cold-finished/hard. Q: What is C.D.W. Boiler Tube? (asked by: montydude123@yahoo.com) A: Cold Drawn Welded Boiler Tube. Q: WHAT IS W.Nr. 1.4301? PLS TELL US IN EASY LANGUAGUE (asked...

[MW:36169] Cold Bending Qualification

Dear Experts,  Can anyone share the inspection requirements or a qualification procedure for cold bending? Our client spec states only the requirements for induction bending and would like to know your opinion on the cold bend inspection requirements. The code of construction is B31.3, Max. 5D bends, A106 SS 316L.  Thanks in Advance. -- https://materials-welding.blogspot.com/ https://www.linkedin.com/groups/122787 --- You received this message because you are subscribed to the Google Groups "Materials & Welding" group. To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com . To view this discussion visit https://groups.google.com/d/msgid/materials-welding/1be61cc3-e9c9-4a5f-834d-e8485e248432n%40googlegroups.com .

[MW:30043] Weep hole

If weep hole is not provided in dummy pipe before welding What will happen??? -- https://materials-welding.blogspot.com/ https://www.linkedin.com/groups/122787 --- You received this message because you are subscribed to the Google Groups "Materials & Welding" group. To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com . To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/da251ee6-fa7f-4851-b876-cdb3834ae341%40googlegroups.com .