Re: [MW:12231] Welding of 45 degree elbows without staggering weld seam

Dear Mr.Ramakrishna ..

It is purely manfacturing mistake and tracebility of Picked Items
....Construction has to check before weld the 2 elbows..If it is not
possible then raise the waiver ...

However In my work experience also I was faced lke this erorrs ,but we
have done 100 % RT and UT for two long seams meeting area ....

Thats All we can do ..In your case PWHT will be added .

Thanks
Suresh

On 8/15/11, limesh M <limesh78@gmail.com> wrote:
> Dear Mr. Carlos,
>
> Could you please mention the corresponding clause as per ASME B31.3 which
> insist fabricator to keep minimum distance(offset) between two long seams
> for better understanding?
>
> Regards,
>
> Limesh
>
> On Sun, Aug 14, 2011 at 3:51 PM, Ramin Kondori
> <raminkondori@gmail.com>wrote:
>
>> What is your material...?
>>
>> If the material is not susceptible to stress relief (like many stainless
>> steels), you can submit a TQ and suggest to carry out stress relief for
>> both
>> parts and then proceed to weld...
>>
>> Regards
>> Ramin Kondori
>> * QC/Welding Engineer *
>> * IWE AT 0070*
>> **
>>
>>
>>
>> On Sun, Aug 14, 2011 at 1:42 AM, carlos oliveros <carlosoliveros@terra.com
>> > wrote:
>>
>>> ASME B31.3 BETWEEN TWO SEAMS LONG MIN IS 1.5 INCH
>>> REGARDS
>>>
>>> Carlos Oliveros
>>>
>>> Mechanical Inspector/ Eng.
>>>
>>>
>>>
>>>
>>> *On vie 12/08/11 13:33 , "Ramakrishna" tv1774@gmail.com sent:
>>> *
>>>
>>> ****************** **
>>>
>>> Dear Friends,****
>>>
>>> Got a case where 2 nos 45 degree elbows are to be welded together and
>>> both
>>> long seams are coinciding without any staggering.****
>>>
>>> There is no provision for welding a pipe piece due to space restriction.*
>>> ***
>>>
>>> Code is ASME/ANSI B31.3****
>>>
>>> Size is 28" dia x 60 mm thick.****
>>>
>>> Joint will be covered by PWHT and NDT is ******Phased array**
>>> **UT****before and after PWHT.
>>> ****
>>>
>>> Can we do this as per code?****
>>>
>>> If yes with what clause/section etc.****
>>>
>>> Please share your opinions.****
>>>
>>> Thanks in advance for your help.****
>>>
>>> Best Regards****
>>>
>>> T.V.Ramakrishna.****
>>>
>>> tv1774@gmail.com ****
>>>
>>> ** **
>>>
>>> --
>>> To post to this group, send email to materials-welding@googlegroups.com
>>> To unsubscribe from this group, send email to
>>> materials-welding+unsubscribe@googlegroups.com
>>> For more options, visit this group's bolg at
>>> http://materials-welding.blogspot.com/
>>> The views expressed/exchnaged in this group are members personel views
>>> and
>>> meant for educational purposes only, Users must take their own decisions
>>> w.r.t. applicable code/standard/contract documents.
>>>
>>> ------------------------------
>>> Este mensaje ha sido verificado por el E-mail Protegido.
>>> Antivirus actualizado en 31/12/1969 / Versión: 0.97/4294967295
>>>
>>>
>>> --
>>> To post to this group, send email to materials-welding@googlegroups.com
>>> To unsubscribe from this group, send email to
>>> materials-welding+unsubscribe@googlegroups.com
>>> For more options, visit this group's bolg at
>>> http://materials-welding.blogspot.com/
>>> The views expressed/exchnaged in this group are members personel views
>>> and
>>> meant for educational purposes only, Users must take their own decisions
>>> w.r.t. applicable code/standard/contract documents.
>>>
>>
>> --
>> To post to this group, send email to materials-welding@googlegroups.com
>> To unsubscribe from this group, send email to
>> materials-welding+unsubscribe@googlegroups.com
>> For more options, visit this group's bolg at
>> http://materials-welding.blogspot.com/
>> The views expressed/exchnaged in this group are members personel views and
>> meant for educational purposes only, Users must take their own decisions
>> w.r.t. applicable code/standard/contract documents.
>>
>
> --
> To post to this group, send email to materials-welding@googlegroups.com
> To unsubscribe from this group, send email to
> materials-welding+unsubscribe@googlegroups.com
> For more options, visit this group's bolg at
> http://materials-welding.blogspot.com/
> The views expressed/exchnaged in this group are members personel views and
> meant for educational purposes only, Users must take their own decisions
> w.r.t. applicable code/standard/contract documents.
>


--
Thanks & Best Regards,

Suresh

Mobile No: 91-92 92 905 905

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

Comments

Popular posts from this blog

Materails FAQs

Q: What are equivalents for standard Q 235 B (and Q 235 A) for U-channels? (asked by: boris.vielhaber@vait.com) A: DIN Nr. = 2393 T.2, 2394 T.2, EN 10025 W. Nr. DIN 17007 = 1.0038 Design DIN 17006 = RSt 37-2, S235JRG2 (Fe 360 B) Q: What is St DIN 2391 BK material? (asked by: dmcandrews@automaticstamp.com) A: Precision steel tubes, cold-finished/hard. Q: What is C.D.W. Boiler Tube? (asked by: montydude123@yahoo.com) A: Cold Drawn Welded Boiler Tube. Q: WHAT IS W.Nr. 1.4301? PLS TELL US IN EASY LANGUAGUE (asked...

[MW:36169] Cold Bending Qualification

Dear Experts,  Can anyone share the inspection requirements or a qualification procedure for cold bending? Our client spec states only the requirements for induction bending and would like to know your opinion on the cold bend inspection requirements. The code of construction is B31.3, Max. 5D bends, A106 SS 316L.  Thanks in Advance. -- https://materials-welding.blogspot.com/ https://www.linkedin.com/groups/122787 --- You received this message because you are subscribed to the Google Groups "Materials & Welding" group. To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com . To view this discussion visit https://groups.google.com/d/msgid/materials-welding/1be61cc3-e9c9-4a5f-834d-e8485e248432n%40googlegroups.com .

Heat tint (temper) colours on stainless steel surfaces heated in air // Heat tint

Introduction The colour formed when stainless steel is heated, either in a furnace application or in the heat affected zone of welds, is dependent on several factors that are related to the oxidation resistance of the steel. The heat tint or temper colour formed is caused by the progressive thickening of the surface oxide layer and so, as temperature is increased, the colours change.   Oxidation resistance of stainless steels However, there are several factors that affect the degree of colour change and so there is no a single table of colour and temperature that represents all cases. The colours formed can only be used as an indication of the temperature to which the steel has been heated. Factors affecting the heat tint colours formed Steel composition The chromium content is the most important single factor affecting oxidation resistance. The higher the chromium, the more heat resistant the steel and so the development of the heat tint colou...