Re: [MW:11422] Official Interpretation for the Vertical Up position qualifies all position

Dear babu,
               In ASME sec.9 as per QW 405 for WPS & PQR positions are non essential variable. for WPQ positions are essential variable.
 
For detail refer QW 405.1,2,3 

On Sat, Jun 18, 2011 at 8:42 PM, K.Babu <kbabupsg@gmail.com> wrote:
Gents,
 
Any one have the official interpretation for the above, as per ASME sec IX or AWS D1.1 for WPS qualification
--
Thanks & regards,

K.Babu

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.



--
THANKS & REGARDS
 
KALYAN VVV
WELDING ENGINEER
THYSSEN KRUPP INDUSTRIES (INDIA) LTD
HYDERABAD
Mob.NO- 09885273257

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

Re: [MW:35289] Welding consumable for S355J2WP material

S355 J2 WP  is a weathering structural steel  It has better atmospheric corrosion resistance. Use E 8018 - W1/W2  Electrodes This is regular...