Re: [MW:11475] Dilution

For this particular question i am suggest you to take chemical analysis for the sample at each 0.5 to 1 mm steps by chipping method. For instant result you have to take multiple points by PMI method.
 


 
On Sat, Jun 25, 2011 at 3:56 PM, Vicky Bangar <bangarvicky007@gmail.com> wrote:
Dear Maulik,

The formula which u have given is correct. But for % of element in weld metal will vary bead by bead. And also for which element shall we calculate? Because element wise laso dilution will change. So in this case what should be taken as reference?

On Fri, Jun 24, 2011 at 9:33 PM, Maulik Thakkar <mlkthakkar2@gmail.com> wrote:
Dear Vicky,
 
Dilution= [% of a element in base metal (by PMI/by TC)-% of a element in weld metal (by PMI/by Chemical testing)-%of a element in filler wire (got it by TC/SEC IIC)] whole divided by % of a element in base metal.
 
Then deduct product from 1 & multiply product to 100.

On Fri, Apr 22, 2011 at 10:23 PM, Vicky Bangar <bangarvicky007@gmail.com> wrote:
Dear sir,
           How to measure dilution in Electroslag Strip Cladding (ESSC)? From macrophotograph it is possible to measure are of diluted base metal and total overlay area. But how to check dilution by chemistry method? How much is percentage dilution expected in ESSC? With higher strip width does dilution changes? What will be effect of base metal thickness on dilution? What are recommended base metal thicknesses for using 60 and 90 wide strips? 

--
Vivek Bangar
B.Tech. Metallurgy and Material Science.
Larsen & Toubro Limited,
Powai

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.



--
Vivek Bangar
B.Tech. Metallurgy and Material Science.
Larsen & Toubro Limited,
Powai

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.



--
Regards,
 
Maulik H. Thakkar
Larsen & Toubro, Hazira

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

Comments

Popular posts from this blog

Materails FAQs

Q: What are equivalents for standard Q 235 B (and Q 235 A) for U-channels? (asked by: boris.vielhaber@vait.com) A: DIN Nr. = 2393 T.2, 2394 T.2, EN 10025 W. Nr. DIN 17007 = 1.0038 Design DIN 17006 = RSt 37-2, S235JRG2 (Fe 360 B) Q: What is St DIN 2391 BK material? (asked by: dmcandrews@automaticstamp.com) A: Precision steel tubes, cold-finished/hard. Q: What is C.D.W. Boiler Tube? (asked by: montydude123@yahoo.com) A: Cold Drawn Welded Boiler Tube. Q: WHAT IS W.Nr. 1.4301? PLS TELL US IN EASY LANGUAGUE (asked...

[MW:36169] Cold Bending Qualification

Dear Experts,  Can anyone share the inspection requirements or a qualification procedure for cold bending? Our client spec states only the requirements for induction bending and would like to know your opinion on the cold bend inspection requirements. The code of construction is B31.3, Max. 5D bends, A106 SS 316L.  Thanks in Advance. -- https://materials-welding.blogspot.com/ https://www.linkedin.com/groups/122787 --- You received this message because you are subscribed to the Google Groups "Materials & Welding" group. To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com . To view this discussion visit https://groups.google.com/d/msgid/materials-welding/1be61cc3-e9c9-4a5f-834d-e8485e248432n%40googlegroups.com .

Heat tint (temper) colours on stainless steel surfaces heated in air // Heat tint

Introduction The colour formed when stainless steel is heated, either in a furnace application or in the heat affected zone of welds, is dependent on several factors that are related to the oxidation resistance of the steel. The heat tint or temper colour formed is caused by the progressive thickening of the surface oxide layer and so, as temperature is increased, the colours change.   Oxidation resistance of stainless steels However, there are several factors that affect the degree of colour change and so there is no a single table of colour and temperature that represents all cases. The colours formed can only be used as an indication of the temperature to which the steel has been heated. Factors affecting the heat tint colours formed Steel composition The chromium content is the most important single factor affecting oxidation resistance. The higher the chromium, the more heat resistant the steel and so the development of the heat tint colou...