Dear yousuf,

I agree with dinesh.it is based on your req.

anyway u can refer ASME B16.25 for butt joint details or asme PV for
joint details depend on your application and stress/design criteria.

for 6mm plate we are doing here single "V " joint.

i think this would helpful.

regards,
mohd.

On Jun 18, 11:02 am, Dinesh Somwanshi <som....@gmail.com> wrote:
> dear yusuf,
>
> it is based on your requirement i.e full penetration or partial , fillet
> weld .
> i think the question is miss some data.
>
> regards
>
> dinesh
>
> On Wed, Jun 15, 2011 at 4:18 PM, yusufkhan pathan <yusufkhan...@gmail.com>wrote:
>
>
>
> > Dear All,
>
> > Can any one please suggest what could be the joint detail for welding of
> > 6mm thk plate.
> > Please refer any code reference if available.
>
> > Regards
> > Yusufkhan.Pathan
> > 8008804165
>
> > --
> > To post to this group, send email to materials-welding@googlegroups.com
> > To unsubscribe from this group, send email to
> > materials-welding+unsubscribe@googlegroups.com
> > For more options, visit this group's bolg at
> >http://materials-welding.blogspot.com/
> > The views expressed/exchnaged in this group are members personel views and
> > meant for educational purposes only, Users must take their own decisions
> > w.r.t. applicable code/standard/contract documents.- Hide quoted text -
>
> - Show quoted text -

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

Re: [MW:35289] Welding consumable for S355J2WP material

S355 J2 WP  is a weathering structural steel  It has better atmospheric corrosion resistance. Use E 8018 - W1/W2  Electrodes This is regular...