Sorry...i mis interpret...If you follow ASME Sec.IX...with this Root WPS you cannot combine ..sine the root pqr should be 13mm and more
Thanks & Regards,
(Karthik)
Karthikeyan.S QA/QC Manager Getabec Energy Co.,Ltd. 379,Moo6,Soi8,Nikhomphatana, Rayong-21180, Thailand. Phone: 0066 38 897035-8 (Off) Fax: 0066 38 897034 Hand Phone: 0066 892512282
--- On Tue, 6/7/11, Karthik <karthik6684@yahoo.com> wrote:
From: Karthik <karthik6684@yahoo.com> Subject: Re: [MW:11267] COMBINATION OF 2 PQR IN ONE WPS To: materials-welding@googlegroups.com Date: Tuesday, June 7, 2011, 11:04 AM
Yes .you can combine as you proposed.
Thanks & Regards,
(Karthik)
Karthikeyan.S QA/QC Manager Getabec Energy Co.,Ltd. 379,Moo6,Soi8,Nikhomphatana, Rayong-21180, Thailand. Phone: 0066 38 897035-8 (Off) Fax: 0066 38 897034 Hand Phone: 0066 892512282
--- On Mon, 6/6/11, manoj john <manojacgnr@gmail.com> wrote:
From: manoj john <manojacgnr@gmail.com> Subject: [MW:11264] COMBINATION OF 2 PQR IN ONE WPS To: materials-welding@googlegroups.com Date: Monday, June 6, 2011, 6:56 PM
Dear All, I have to weld 40 mm thk ss 304 plate to be welded with root GTAW and subsequent run by SMAW. I have 2 WPS,one WPS GTAW + SMAW thickness range qualified is 1.6 to 12 mm and another procedure qualified 5 mm to 50 mm with back gouging. My doubt is can i make one wps supporting with these 2 Procedure Root with GTAW and subsequent run with SMAW so i can carry out the welding with GTA + SMAW 40 mm thk without further procedure qualification. Thanks & Regards. Manoj -- To post to this group, send email to materials-welding@googlegroups.comTo unsubscribe from this group, send email to materials-welding+ unsubscribe@googlegroups.comFor more options, visit this group's bolg at http://materials-welding.blogspot.com/The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
| -- To post to this group, send email to materials-welding@googlegroups.com To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com For more options, visit this group's bolg at http://materials-welding.blogspot.com/ The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
|
--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at
http://materials-welding.blogspot.com/ The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
No comments:
Post a Comment